| Stacking Fault in γ’ Precipitate of Single Crystal Nickel Base Superalloy DD8 After Out-of-Phase Thermo-Mechanical Fatigue |
| WANG Yuechen; LI Shouxin; AI Suhua; LIU Feng; ZHOU Li; ZHANG Hui |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
WANG Yuechen; LI Shouxin; AI Suhua; LIU Feng; ZHOU Li; ZHANG Hui. Stacking Fault in γ’ Precipitate of Single Crystal Nickel Base Superalloy DD8 After Out-of-Phase Thermo-Mechanical Fatigue. Acta Metall Sin, 2003, 39(2): 150-154 .
[1] Khan T, Caron P. High Temperautre Materials for PowerEngineering. Part II, The Netherland Kluwer: Academic.Publishers, 1990: 1661 [2] Zhang J H, Xu Y B, Wang Z G. Scr Metall Mater. 1995;32: 2093 [3] Tian S G. Ph.D. Dissertation, Shenyang, NortheasternUniversity, 1998(田素贵.东北大学博士学位论文,沈阳, 1998) [4] Zhang J H, Hu Z Q, Xu Y B, Wang Z G. Metall Trans.1992; 23A: 1253 [5] Shaikh M A, Xu Y B, Hu Z Q. Metall Sci Technol, 1999;17: 53 [6] Mukherji D, Jiao F, Chen W, Wahi R Q. Ada MelallMater, 1991; 39: 1515 [7] Brigitte D, Allan J M. Philos Mag, 1991; 64A: 641 [8] Lall C, Chin S, Pope D P. Metall Trans, 1979; 10A: 1323 [9] Shah D M, Duhl D N. Proc 5th Int Symp on Super-alloys,Warrendale: Metallurgical Society of AIME, 1984: 105 [10] Brigitre D, Allan J M. Philos Mag, 1991; 64A: 641 [11] Li Y Q, Liu J Y. Precipitate of Grain Boundary of Super-alloy. Beijing: Metallurgy Industry Press, 1976: 310(李玉清,刘锦岩,高温台金的晶界间隙相。北京:冶金工业出版社, 1976:310) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|