Please wait a minute...
Acta Metall Sin  2003, Vol. 39 Issue (2): 140-144     DOI:
Research Articles Current Issue | Archive | Adv Search |
Numerical Simulation of Channel Segregation in Vertically Unidirectional Solidification Process
HAN Zhiqiang; LIU Baicheng
Department of Mechanical Engineering; Tsinghua University; Beijing 100084
Cite this article: 

HAN Zhiqiang; LIU Baicheng. Numerical Simulation of Channel Segregation in Vertically Unidirectional Solidification Process. Acta Metall Sin, 2003, 39(2): 140-144 .

Download:  PDF(197KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  15 April 2002     
ZTFLH:  TG111.4  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I2/140

[1] Giamei A F, Kear B H. Metull Trans, 1970; I: 2185
[2] Copley S M, Giamei A F, Johnson S M, Hornbecker M F.Metall Trans, 1970; 1: 2193
[3] Sample A K, Hellawell A. Metall Trans, 1984;15A: 2163
[4] Neilson D G., Incropera F P. Int J Heat Mass Transfer,1991; 34: 1717
[5] Felicelli S D, Heinrich J C, Poirier I) R. Metall Trans,1991; 22B; 847
[6] Schneider M C, Gu J P. Beckermann C, Boettingnr W J,Kattner U R. Metall Mater Trans, 1997; 28A: 1517
[7] Felicelli S D, Poirier D R, Heinrich J C. Metall Mater Trans, 1998; 29B: 847
[8] Bennon W D, Incropera F P. Int J Heat Mass Transfer,1987; 30: 2161
[9] Han Z Q, Shen H F, Xiong S M, Liu B C. Ada MetallSin, 2002; 38: 941(韩志强,沈厚发,熊守美,柳白成.金属学报,2002;38:941)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!