Please wait a minute...
Acta Metall Sin  2003, Vol. 39 Issue (1): 94-98     DOI:
Research Articles Current Issue | Archive | Adv Search |
The EIS Analysis of Cathodic Reactions During CO2 Corrosion of N80 Steel
CHEN Changfeng; LU Minxu; ZHAO Guoxian; BAI Zhenquan; YAN Milin; YANG Yanqing
School of Materials Science of Engineering; University of Science of Technology Beijing; Beijing 100083
Cite this article: 

CHEN Changfeng; LU Minxu; ZHAO Guoxian; BAI Zhenquan; YAN Milin; YANG Yanqing. The EIS Analysis of Cathodic Reactions During CO2 Corrosion of N80 Steel. Acta Metall Sin, 2003, 39(1): 94-98 .

Download:  PDF(180KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  29 March 2002     
ZTFLH:  TG172  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/94

[1] Schmitt G. In: Hausler R H, Giddard H P eds, Advances in CO2 Corrosion, Vol.1, Houston, Texas: NACE, 1984:1
[2] Ikeda A, Ueda M, Mukai S. In: Hausler R H, Giddard H Peds, Advances in CO2 Corrosion, Vol. 1, Houston, Texas:NACE, 1984: 39
[3] Videm K. Predicting CO2 Corrosion in the Oil and GasIndustry, Working Party Report. London: The Instituteof Materials, 1994: 144
[4] Waard C D, Milliams D E. Corrosion, 1975; 31(5) : 177
[5] Schmitt G. Corrosion 83, Houston: NACE 1983: 43
[6] Ogundele G I, White W E. Corrosion, 1986; 42(2) : 71
[7] Xa Z, Chou K C, Smialowska Z S. Corrosion, 1989; 45(8) :636
[8] Nesic S, Postlethwaite J, Olsen S. Corrosion, 1996; 52(4) :280
[9] Zhang X Y, Yu G, Wang F P, Du Y L. Chem J Chin Univ,1999; 20: 1115(张学元,余刚,王凤平,杜元龙.高等学校化学学报,1999;20:1115)
[10] Linter B R, Burstein G T. Corro Sci, 1999; 42(2) : 117
[11] Cao C N. Electrochimica Acta, 1990; 35: 831
[12] Cao C N. J Chin Soc Corros Prot, 1993; 13: 91(曹楚南.中国腐蚀与防护学报, 1993;13:91)
[13] Li J, Lu M X, Yan M L, Zhao G X, Sun D B, Yang D J. J Chin Soc Corros Prot, 1999; 19: 285(李静,路民旭,严密林,赵国仙,孙东柏,杨德钧.中国腐蚀与防护学报,1999;19:285)
[14] Cao C N. Corrosion Electrochemistry. Beijing: Chemical Industry Press, 1995: 103(曹楚南.腐蚀电化学.北京:化学工业出版社, 1995:103)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!