Please wait a minute...
Acta Metall Sin  2003, Vol. 39 Issue (1): 89-93     DOI:
Research Articles Current Issue | Archive | Adv Search |
Investigation of the Structure and the Property of Hydrogen Storage Ti-Mo Alloys
ZHAO Yue; ZHENG Hua; LIU Shi; YANG Rui; WANG Longbao
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

ZHAO Yue; ZHENG Hua; LIU Shi; YANG Rui; WANG Longbao. Investigation of the Structure and the Property of Hydrogen Storage Ti-Mo Alloys. Acta Metall Sin, 2003, 39(1): 89-93 .

Download:  PDF(162KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  07 March 2002     
ZTFLH:  TG146.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/89

[1] Nakahara K, Tokumoto K, Sakaguchi S, Hayashi Y. J JpnSoc Powder Powder Metall, 1998; 45: 769
[2] Xia K H, Schen R, Jr., Ho J C. Chim Phy, 2000; 38: 205
[3] Ho W F, Ju, C P, Lin J H. Biomaterials, 1999; 20: 2115
[4] Shi L, Zhou Z, Zhao G. Acta Metell Sin, 2000; 36: 530(施利群,周筑颖,赵国庆.金属学报, 2000;36:530)
[5] Young G A Jr, Scully J R. Scr Metall Mater, 1993; 28:507
[6] Gao S, Yu B. J Functional Mater(supple), 2001; 32: 999(高树俊,虞炳西.功能材料(增刊),2001;32:999)
[7] Yang R, Wang Y M, Zhao Y, Wang L B, Ye H Q, WangC Y. Acta Met, 2002; 50: 109
[8] PCPDFWIN, VERSION 1. 10. September, JCPDS-TCDD,1995
[9] Wrongski Z S. Int Mater Rev, 2001; 46: 1
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!