Effect of Be on the Age-Hardening Characteristics of As-Cast Al-11Si-0.3Mg Alloy |
WANG Guiqing; BIAN Xiufang; ZHANG Junyan |
Key Laboratory of Liquid Structure and Heredity of Materials; Ministry of Education; Shandong University; Jinan 250061;Department of Material Science and Technology; Shandong architectural engineering institute; Jinan 250014 |
|
Cite this article:
WANG Guiqing; BIAN Xiufang; ZHANG Junyan. Effect of Be on the Age-Hardening Characteristics of As-Cast Al-11Si-0.3Mg Alloy. Acta Metall Sin, 2003, 39(1): 43-46 .
[1] Shivkumar S, Keller C, Apelian D. AFS Trans, 1990; 98:905 [2] Kang H G, Kida M, Miyahara H, Ogi K. AFS Trans, 1999;107: 507 [3] Kaczorowski M, Bindas J. Aluminium, 1994; 9/10: 566 [4] Crowell N, Shivkumar S. AFS Trans, 1995; 103: 721 [5] Caceres C H, Wang Q G. AFS Trans, 1996; 104: 1039 [6] Shivkumar S, Wang L, Keller C. AFS Trans, 1995; 103:705 [7] Bailey W A. J Inst Met, 1967; 95: 443 [8] Ouellet P, Samuel F H. J Mater Sci, 1999; 34: 4671 [9] Murali S, Raman K S. Cast Met, 1991; 4: 31 [10] Gregson P J, Flower H M, Tite C N J. Mater Sci Technol,1986; 2: 349. [11] Xiao T, Youdelis W V. Mater Sci Technol, 1989; 5: 991 [12] Youdelis W V, Fang W. Mater Sci Technol, 1994; 10: 1031 [13] Zhen 1, Fei W D, Kang S B. J Mater Sci, 1997; 32: 1895 [14] Eskin D G, Massardier V, Merle P A. J Mater Sci, 1999;34: 811 [15] Malinov S, Guo Z. Metall Mater Trans A, 2001; 32A: 879 [16] Xu Z Y. The Theory of Phase Transformations. Beijing: Science Press, 1988: 32(徐祖耀.相变原理.北京:科学出版社, 1988:32) [17] Friend C M, Luxton S D. J Mater Sci, 1988; 23: 3173 [18] kim T S, kim T H, Oh K H, I.Lee H. J Mater Sci, 1992;27: 2599 [19] Samuel A M, Samuel F H. AFS Trans, 1994; 102: 397x |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|