Cite this article:
. . Acta Metall Sin, 1999, 35(2): 147-151 .
|
|
Received: 23 October 1998
|
|
[1] Lubanska H. J Met, 1970; 22(2). 45 [2] Grant P S, Maher P, Cantor B. Mater Sci Eng, 1994;A179/A180: 72 [3] Fu X W, Zhang J S, Sun Z Q. J Univ Sci Technol Beijing,1998; 16(in press)(傅晓伟,张济山,孙祖庆。北京科技大学学报, 1998; 16(已接收)) [4] Szekely J, Themelis N. Wiley (New York), 1971; 170: 661 [5] Hurth J P. Metall Tran, 1978; 9A: 401 [6] Mathur P, Apelian D, Lawley A. Acta Metall Mater, 1989;37: 429 [7] Fritsching U, Zhang H, Bauchkhage K. Steel Res, 1994; 65(7):273 [8] Fu X W, Zhang J S, Yang W Y, Sun Z Q, In: Imam M A,Denale R, Harada S, Zhang Z, Lee D N eds., The PRICM3on Advanced Materials and Processing. USA: The Minerals,Metals & Materials Society, 1998; 12: 1713Z |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|