Cite this article:
. . Acta Metall Sin, 1999, 35(10): 1107-1111 .
[1] He Y D Sahai Y. Metall Truns, 1987; 18B: 81 [2] HE Y D, Sahai Y. Acta Metall Sin, 1989; 25: B272 (贺友多, Sahai Y.金属学报,1989; 25: B272) [3]Joo S Guthrie R I L. Metall Trans, 1993; 24B: 755 [4] Jones W P, Launder B E. Int J Heat Mass Transf, 1973; 16:1119 [5] Ilegbusi O J.Szekely J.Mathematical Modeling of Materials Processing Operations.Warrendale Warrendale,PA:TMS,1987:409 [6] Shirabe K. A Mathematical Model of RH Vacuun Degassing System. M.Sc. Thesis, Massachusetts Institute of Technol ogy 1981 [7] Lee S M, Koo Y S, Kang T, Lee I R Shin Y K. Proc 6th Int Iron and Steel Cong, Tokyo: ISIJ, 1990: 239 [8] Sahai Y, Emi T. ISIJ Int, 1996; 36: 1116 |