THE PREPARATION OF IRON CARBIDE BY GAS REDUCTION
WANG Guanghui; JIANG Maofa; WANG Wenzhong(Department of Ferrous Metallurgy; Northeastern Universityt Shenyang 110006)
Cite this article: 

WANG Guanghui; JIANG Maofa; WANG Wenzhong(Department of Ferrous Metallurgy; Northeastern Universityt Shenyang 110006). THE PREPARATION OF IRON CARBIDE BY GAS REDUCTION. Acta Metall Sin, 1998, 34(7): 769-773.

Download:  PDF(406KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Influences of temperature and composition of CO-CO2-H2 gas mixtures on the formation rate of iron carbide during iron ore reduction are discussed through thermodynamic calculation and corresponding experiments. Based on the examination of the composition of reduction products, the feasibility is confirmed for the preparation of iron carbide by CO-CO2-H2gases reducing iron ore.
Key words:  iron carbide      gas reduction      carbon deposition     
Received:  18 July 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I7/769

1金国范.炼钢,19942 10(2):62 (Jin Guofan.Steelmaking,1994; 10(2):62)
2 Stephens F A Jr. Steel Times Int, 1993; 17(3): 11
3 Smithyman C M. Iron Steel Eng, 1996; 73(8): 48
4 Correnti J D. Ironmaking Conf Proc, 1993; 52: 347
5 Garrawav R. Iron Steelmaker. 1996: 23(6): 27
6 梁英教,车荫昌.无机物热力学数据手册沈阳:东北大学出版社,1993:458(Liang Yingjiao, Che Yinchang.Thermodynamical Data Handbook of Inorganic Compounds. Shenyang: Northeastern University Press,1993:458)&
No related articles found!
No Suggested Reading articles found!