Abstract ZnO voltage-sensitive ceramics doped with some metal chides were prepared by coprecipitation. The optimal preparing condition was determined as follows: reaction pH value of 6.90 ± 0.05, calcining temperature of 500 ℃, sintering temperature of 1100 ℃. Varistor ceramics made from coprecipitating powders showed improved electrical properties and stability to temperature. The powders were also examined by SEM, IR and XRD etc. The mechanism of zinc oxide ceramics showing the voltage sensitive characteristic has been discussed to some extent.
1 Van Kemenade J T G, Eijnthove R K. J Appl Phys, 1979; 50: 938 2 Schwing U, Hoffmann B. J Appl Phs, 1985; 57: 5372 3 Hall D C, Leach C. J Mater Sci, 1995; 30: 2733 4 Philip H R, Levinson L M. J Appl Phys, 1981; 52: 1083 5 周宏庆.功能材料,1996;27(1):50 (Zhou Hongqing、 Funct Mater, 1996 27(1): 50) 6 Lauf R J, Bond W D. Am Ceram Soc Bull, 1984; 63: 278 7 Hshita S, Yao Y, Shirasaki M. J Am Ceram Soc, 1989; 72: 338 8 Hohenberger G, Tomandl G. J Mater Res, 1992; 7: 546 9 徐跃萍,郭景坤硅酸盐学报,1992;20(1):35 (Xu Yueping,Guo Jingkun.J Chin Ceram Soc;1992 20(1):35) 10 陈允魁红外吸收光谱法及应用上海:上海交通大学出版社,1993:137(Chen Yunkui. IR Absorntion Spectrometry and Application. Shanghai: Shanshai Jiaotong University Publishing House; 1993: 137) 11 李慧峰,许毓春,王礼琼,王士良压电与声光,1994;16(6):27(Li Huifeng,Xu Yuchun,Wang Liqiong,Wang Shiliang.Piezoelectric Acoustooptics,1994; 16(6):27)