COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS
CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS. Acta Metall Sin, 1998, 34(4): 423-430.

Download:  PDF(805KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The computer simulation of magnetization process of a single powder particle of the Nd2Fe14B/α-Fe nanocomposite magnet has been performed. Three types of hysteresis loops have been observed at different conditions: Stoner-Wohlfarth like type, contracted loop and normal hysteresis loop with a good rectangularity. The behavior of the reduced remanence, the intrinsic coercivity and the change of maximum magnetic energy product with the grain size, a,and the content of the soft phase, fm, have been studied. For the model nanocomposite magnetsof fm=40% and the grain size a=25 nm, the optimum value of (BH)max=375 kJ/m3 is attained.It is remarkably enhanced in comparison with the maximum of (BH.)max=264 kJ/m3 of the pure Nd-Fe-B magnet.
Key words:  nanocomposite magnet      exchanged interaction      computer simulation     
Received:  18 April 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I4/423

1 McCallum R W, Kadin A M, Clemente G B, Keem J E. J Appl Phys, 1987; 61: 3577
2 Manaf A, Buckley R A, Davies H. J Magn Magn Mater, 1993; 128: 302
3 Kneller E P, Hawig R. IEEE bens Magn, 1992; MAG-27: 3588
4 Skomski R, Coey J M D. Phys Rev, 1993; 48B: 15812
5 Schrefl T, Fidler J, Kronmller H. Phys Rev, 1994; 49B: 6100
6 Liu W, Wang Q, Sun X K, Zhao X G, Zhao T, Zhang Z D, Chuang Y C. J Magn Magu Mater, 1994; 131: 413
7 Yang J L, Wang Q, Sun X K, Zeng G Y, Chen M, Liu W, Zhao X G, Zhso T, Zhang Z D. J Mop Magn Maten 1994; 134: 197
8 Jin Z Q, Sun X K, Liu W, Zhao X G, Xiao Q F, Sui Y C, Zhang Z D, Wang Z G, Qin H X. i Magn Magn Mater, 1997; 169: 135
9 Fukunaga H, Inoue H. Jpn J Appl Phgs, 1992; 31: 1347
10 Binder K, Heermann D W 著 秦克诚译. 统计物理学中的蒙特罗模拟方法. 北京:北京大学出版社, 1994: 33 (Binder K, Heermann D W ed, Qin Kecheng trans. Monte Carlo Simulation in Statistical Physics. Beijing:Peking Uni Press, 1994; 33)
11 Zijlstra H. In: Wohlfarth E P ed., Fermmagnetic Materiats, Vol.3., Amsterdam: N0rth-Holland Publishing, 1982: 37
12 Kronmller H. In: Long G J, Grandjcan F eds., Supermaguets, Hard Manetic Materiais, Dordrecht:Kluwer Academic Publisherrs, 1990: 461
13 Chudnovsky E M, In: Fernandez-baca J A, Ching Wai-Yim eds., The Manetism of Amorphous Metais and Alloys. Singapore: World Scientific, 1995: 143
14 Herzer G. IEEE Trans Magn, 1990; MAG-26: 1397
15 Otani Y, Li H S, Coey J M D. IEEE Trans Magn, 1990; MAG-26: 2658
[1] Dianguo MA,Yingmin WANG,Kunio YUBUTA,Yanhui LI,Wei ZHANG. Effect of Co Content on the Structure and Magnetic Properties of Melt-Spun Fe55-xCoxPt15B30 Alloys[J]. 金属学报, 2017, 53(5): 609-614.
[2] ;. STUDY OF 3D QUASI--STATIONARY GRAIN SIZE DISTRIBUTION DERIVED FROM MACPHERSON—SROLOVITZ TOPOLOGY--RELATED GRAIN GROWTH RATE EQUATION[J]. 金属学报, 2008, 44(7): 769-774 .
[3] zhang lin. Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics[J]. 金属学报, 2008, 44(10): 1161-1166 .
[4] HOU Hua; ZHAO Yuhong; CHEN Zheng; XU Hong. Prediction for the Early Precipitation Process of Ni75AlxV25-X System with Lower Al Concentration by the Phase-Field Model[J]. 金属学报, 2005, 41(7): 695-702 .
[5] ZHANG Lin; ZHANG Caibei; WANG Yuanming; WANG Shaoqing. Cellular Automaton Modelling Of The Transformation From Austenite to Ferrite In Low Carbon Steels During Continuous Cooling[J]. 金属学报, 2004, 40(1): 8-13 .
[6] SUI Zhitong;ZHANG Peixin(Northeastern University; Shenyang 110006). SELECTIVE PRECIPITATING BEHAVIOR OF THE BORON COMPONENTS FROM THE BORON SLAGS[J]. 金属学报, 1997, 33(9): 943-951.
[7] YIN Aijun; LI Jing; LI Hinhai; HUANG Kexiong; JIANG Hanying (Central South University of Technology; Changsha 410083) (Manuscript received 1995-06-30; in revised form 1995-12-01). COMPUTER SIMULATION ON MINOR ELEMENT BEHAVIOUR IN COPPER FLASH SMELTING[J]. 金属学报, 1996, 32(4): 387-392.
[8] CAI Xun; ZHOU Pingnan; (Shanghai Jiaotong University ; Shanghai 200030)Bangert H (Technical University of Vienna; Auslria)(Manuscript received 94-07-18). SIMULATION OF INDENTATION MICROHARDNESS TESTING[J]. 金属学报, 1995, 31(13): 44-5.
[9] CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology). COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT[J]. 金属学报, 1994, 30(24): 537-542.
[10] CHEN Da;LU Min;LIN Dongliang (Lin T L) Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai Jiao Tong University; Shanghai 200030. SIMULATIVE STUDY OF INTERACTION BETWEEN GRAIN BOUNDARIES AND DISLOCATIONS IN Ni_3Al[J]. 金属学报, 1993, 29(7): 34-39.
[11] SHAO Jun;XU Hua;CHENG Ailan;KLEIN M. L. University of Pennsylvania; Philadelphia; U. S. A; State University of New York; U. S. A.; University of Pennsylvania; Philadelphia; U. S. A.. CONSTANT PRESSURE MOLECULAR DYNAMICS SIMULATION OF MOLTEN LiF-BeF_2 SYSTEM[J]. 金属学报, 1993, 29(1): 59-64.
[12] YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology. SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM[J]. 金属学报, 1991, 27(5): 8-13.
[13] WANG Xi;ZHOU Jiankun;CHEN Youshan;LIU Xianghuai;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia Sinica. COMPUTER SIMULATION OF ION BEAM ENHANCED DEPOSITION OF TiN FILMS[J]. 金属学报, 1991, 27(3): 136-141.
[14] WEI Chao;QIAN Rengen;LIN Shi;XIAO Jimei University of Science and Technology Beijing Department of mathematics and mechanics; University of Science and Technology Beijing; Beijing 100083. COMPUTER SIMULATION OF EFFECT OF ORIENTATION DIFFERENCE ON MECHANICAL PROPERTIES OF BICRYSTALLINE SPECIMENS[J]. 金属学报, 1990, 26(4): 18-21.
[15] LIN Dongliang;CHEN Da T. L. Lin Shanghai Jiaotong University professor;Department of Materials Science;Shanghai Jiaotong University;Shanghai 200030. COMPUTER SIMULATION OF GRAIN BOUNDARY STRUCTURES IN Ni_3 Al[J]. 金属学报, 1990, 26(3): 10-17.
No Suggested Reading articles found!