OSCILLATORY COUPLING OF THE Co-Nb/Cr MULTILAYERED FILMS
LOU Jianxin; YAN Shishen; LIU Yihua (Department of physics; Shandong University; Jinan 250100)
Cite this article: 

LOU Jianxin; YAN Shishen; LIU Yihua (Department of physics; Shandong University; Jinan 250100). OSCILLATORY COUPLING OF THE Co-Nb/Cr MULTILAYERED FILMS. Acta Metall Sin, 1998, 34(4): 412-415.

Download:  PDF(394KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Co-Nb/Cr multilayered films were prepared with the rf-sputtering method. The magnetic properties of the samples were studied by a micropro cessor-controlled vibrating-sample magnetometer. When the charging Ar pressure PAr=2.67 Pa, an oscillation between ferromagnetic and antiferromagnetic coupling with the thickness of Cr layers was found, and the spontaneous magnetization Ms remains constant basically. When PAr=0.67 Pa, the value of Ms shows an oscillatory behaviour, which may be related to the oscillatory variation of the paramagnetic component in the ferromagnetic layers.
Key words:  muiltilayered film      ferromagnetic coupling      antiferromagnetic coupling     
Received:  18 April 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I4/412

1 Grunberg P, Schreiber R, Pang Y, Brodsky M B, Sowers H. Phys Rev Lett, 1986; 57: 2442
2 Barthlmy A, Fert A, Baibich M N, Hadjoudj S, Petroff F, Etienne P, Cabanel R, Lequien S, Nguyen Van Dan F, Creuzet G. J Appl Phys, 1990; 67: 5908
3 Parkin S S P, Bhadra R, Roche K P. Phys Rev Lett, 1991; 66: 2152
4 Celinski Z, Heinrich B. J Magn Magn Maten 1991; 99: L25
5 Parkin S S P, More N, Roche K P. Phys Rev Lett, 1990; 64: 2304
6 Qiu Z Q. Pearson J, Berger A, Bader S D. Phys Rev Lett, 1992; 68: 1398
7 FuB A, Demokritov S, Grunberg P, Zinn W. J Magn Magn Maten 1992; 103: L221
8 Levy M, Ounadjela K, Zhang S, Wang Y, Sommers C B, Fert A. J Appl Phys, 1990; 67: 5914
9 Bruno P, Chappert C. Phys Rev Lett, 1991; 12: 1602
10 Toscano S, Briner B, Hopster H, Landolt M. J Magn Magn Mater, 1992; 114: L6
11 Liu Y H, Zhang Y M, Yan S S, Ma X D. Phys Rev, 1993; B8: 10266
12 谭春雨, 夏日源, 张汝贞, 刘吉田, 刘向东, 许炳章, 李淑英, 陈友鹏, 绑淑芝. 山东大学学报, 1993; 28: 189(Tan C Y, Xia Y Y, Zhang R Z, Liu J T, Liu X D, Xu B Z, Li S Y, Chen Y P, Zhang S Z. i Shandong Uni,1993; 28: 189)
13 Baibich M N, Broto J M, Fert A, Nguyen Van Dan F, Petroff F, Etienne P, Creuzet G, niederich A, ChazelasJ. Phys Rev Lett, 1988; 61: 2472
No related articles found!
No Suggested Reading articles found!