LATTICE CONSTANTS OF DISORDERED AND ORDERED PHASES IN Au-Cu SYSTEM
XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; Changsha 410083)Correspondent:XIE Youqing; professor; Tel: (0731)8879287; Fax. (O731)8826136Manuscript received 1997-11-14; in revised form 1998-02-12
Cite this article: 

XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; Changsha 410083)Correspondent:XIE Youqing; professor; Tel: (0731)8879287; Fax. (O731)8826136Manuscript received 1997-11-14; in revised form 1998-02-12. LATTICE CONSTANTS OF DISORDERED AND ORDERED PHASES IN Au-Cu SYSTEM. Acta Metall Sin, 1998, 34(12): 1233-1242.

Download:  PDF(776KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

According to characteristic crystal theory of alloy phases, atomic state of acomponent is split into some characteristic atomic states in the solid solution. Lattice constantsof alloys may be obtained by characteristic lattice constaat additive law, characteristic atomicvolume additive law and characteristic atomic state additive law, but they are not equal in value.Nine lattice constant functions of disordered binary solid solutions are introduced. The functionssuitable for disordered An-Cu alloys and their components have been determined. Lattice constats of Au3Cu, AuCu, AuCu3 and relevant ordered alloys as a function of composition havebeen pradicated. Theoretical values are in good agreement with eXperimental values.

Key words:  An-Cu system      disordered alloy      ordered alloy      lattice constant      atomic volume     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I12/1233

1谢佑卿,马柳莺.中南矿冶学院学报,1985;3:1(Xie Y Q, Ma L Y.J Central-South Inst Min Metall,1985;3: 1)
2 Vegard L. Z PhyS, 1921; 5: 17
3 Zen E-an. Am Mineral,1956; 41: 523
4谢佑卿,马柳莺中南矿冶学院学报,1985;1:1(Xie Y Q, Ma L Y J Cent South Iust Min Metall, 1985; 1: 1)
5 Lupis C H P, Elliott J F. Acta Metall, 1967; 15: 265
6 Xie Y Q. Acta Metall Matet 1994; 11:3705
7谢佑卿,张晓东,陈嘉砚中国科学,1996;E26:224(Xie Y, Zhang X D, Chen J Y. Sci Chin, 1996; E39: 394)
8 谢佑卿.中国科学,19972:E27:488(Xie Y Q.SCi Chin,1998; E41:146)
9 Okamoto H, Chakrabarti D J, Laughlin D E, Massalski T B Bull Alloy Phase Diagrams.1987; 8: 454
10谢佑卿,张晓东金属学报, 1994; A30: 531(Xie Y Q, Zhang X D. Acta Metall Sin, 1994; A30: 531)
11Pearson W B.Handbook of Lattice Spacings and Structure of Metals and alloys.London:Pergamon,1958:411
12 Johannsson C H, Linde J O Ann Phys, 1936 25: 1
13 Okamura K, Iwasaki H, Ogawa S j Phys Soc jpn, 1968; 24: 569
14 Flinn P A, McManus G M, Rayne J A J Phys Chem Solids, 1960; 15: 189
[1] WANG Youdao WU Erdong WANG Sucheng LI Wuhui. X-RAY DIFFRACTION ANALYSIS ON THE THICKNESS EFFECT OF γ/γ' LATTICE MISMATCHE IN NICKEL BASE SINGLE CRYSTAL SUPERALLOY DD10[J]. 金属学报, 2011, 47(11): 1418-1425.
[2] XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; ChangSha 410083)CorrsPondent: XIE Youqing; pwtsson Tel: (O731)8879287; Fax: (0731)8826136Manuscript received 1997-12-1; in revised form 1998-0406. RELATIONSHIP BETWEEN PARTIAL AND AVERAGE ATOMIC VOLUMES OF COMPONENTS IN Cu-Ni ALLOYS[J]. 金属学报, 1998, 34(12): 1243-1248.
[3] LIN Junpin;CHU Wuyang;XIAO Jimei(University of Science and Technology Beijing). STRESS CORROSION CRACKING AND HYDROGEN INDUCED CRACKING OF ORDERED B_2-TYPE Fe_3Al[J]. 金属学报, 1994, 30(2): 85-90.
[4] XIE Youqing;ZHANG Hiaodong(Central South University of Technology; Changsha). MICROSTRUCTURE AND PROPERTIES OF Au-Cu ALLOYS[J]. 金属学报, 1994, 30(12): 531-539.
[5] XU Wenchong;SUN Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing XU Wenchong; senior engineer; Department Institute; Ministry of Metallurgical Industry No;13. Central Iron and SteelResearch Beijing 100081. LATTICE PARAMETERS OF COMPLEX CARBONITRIDE CONTAINING Ti, Nb AND V[J]. 金属学报, 1989, 25(6): 146-148.
No Suggested Reading articles found!