EXTENDING OF THE SOLID SOLUBILITY OF Fe-Cu NANO-POWDER THROUGH ADDING MINOR BORON
XU Yuseng; JIANG Huanhong; QIAN Min; JIN Zongming; WANG Yaorong; QIU Guoyang; MA Rongbing; XUE Qing (Suzhou University; Suzhou 215006)(Manuscript received 1996-09-05; in revised form 1996-10-30)
Cite this article: 

XU Yuseng; JIANG Huanhong; QIAN Min; JIN Zongming; WANG Yaorong; QIU Guoyang; MA Rongbing; XUE Qing (Suzhou University; Suzhou 215006)(Manuscript received 1996-09-05; in revised form 1996-10-30). EXTENDING OF THE SOLID SOLUBILITY OF Fe-Cu NANO-POWDER THROUGH ADDING MINOR BORON. Acta Metall Sin, 1997, 33(8): 807-813.

Download:  PDF(668KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The nanometre-sized Fe-Cu supersaturated solid solutions were prepared by chemical reduction. There is a small amount of boron dissolved in the alloys. The solid solu-bility of fcc-phase is largely extended to about an atomic ratio of 4: 1 for Fe and Cu. The range of fcc phase in the Fe-Cu alloy goes beyond the scope of that prepared by mechanical alloying. The fcc phase was found to be rather stable during heat treatment. The large solubil-ity extending and high stability of fcc phase are caused by the small amount of boron con-tained in the alloys.
Key words:  chemical reduction      Fe-Cu alloysupersaturated solid solution     
Received:  18 August 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I8/807

1 Campbell S J, Clark P E. J Phys F: Metal Phys, 1974; 4:1073
2 Kneller E F. J APH Phys,1964; 35:2210
3 Chien C L, Liou S H, Kofalt D, Yu Wu, Egami T, McGuire T R. Phys Rev,1986; B33: 3247
4 Eckert J, Holzer J C, Johnson W L. J Appl Phys,1993; 73:131
5 Eckert J, Holzer J C, Krill C E, Johnson W L. J APd Phys, 1993, 73: 2794
6杨元政,马学鸣,董远达.金属学报,1992; 28:399
7齐民,朱敏,杨大智.材料科学进展, 1993; 7: 31
8韦世强,殷士龙,刘文汉,刘方新,高琛,杨元政,董远达,胡天斗.物理学报,1994; 43: 1630
9 Brandes E A. Smithells Metals Reference Book. Sixth Edition, London: Butterworth,1983:11
10 Van Wonterghern J, Morup S, Koch C J W, Charles S W. Nature, 1986; 322: 622
11 Wells S, Charles S W, Morup S, Linderoth S, van Wonterghem J, Larsen, Madsen M B. J Phys,1989; Cl: 8199
12 Xu Yusheng, Yang Xiangqing, Wu Xucmei, Ye Chao, Jiang Huali. Hyper fine Interact, 1991; 69:681
13 Xu Song, Xu Yusheng, Jiang Huali, Xue Qing. Nucl Instrum and Methods Phys Res,1993; B76: 260
14 Jiang J Z, Gonser U, Gente C and Bormann R. APd Phys Lett, 1993, 63. 1056
15 Polk D E. Acta Metall, 1972; 3: 484
16郭贻诚,王震西.非晶态物理学.北京:科学出版社,1984:68
17 Cahn R W,Haasen P.Physcal Metallurgy,3rd ed,Amsterdam:Elsevier Sci Publ,1983:980
18隋曼龄,卢柯.金属学报,1994;30:B413
[1] LV Dongsheng; LI Weishan; TAN Chunlin; ZE Ronghua. PREPARATION AND ELECTROCHEMICAL BEHAVIORS OF Co-B ALLOY POWDERS[J]. 金属学报, 2010, 46(3): 346-351.
[2] ;. Investigation on Preparation of Tb2Fe17 by Direct Electrochemical Reduction of Tb4O7-Fe2O3 Pellet in Molten Calcium Chloride[J]. 金属学报, 2008, 44(7): 859-862 .
No Suggested Reading articles found!