| KPO_3-M0O_3 PHASE DIAGRAM |
| FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10) |
|
Cite this article:
FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM. Acta Metall Sin, 1997, 33(4): 395-397.
|
|
|
Abstract The phase diagram of KPO3-MoO3 binary system has been determined by means of visual polythermal, DTA and X-ray diffraction analyses. It was found that two compounds formed in this binary system, their stoichiometrical formula are KPO3MoO3 and 3KPO3 MoO3, respectively. The existence of two compounds has been also proved by Raman spectrum analysis.
|
|
Received: 18 April 1997
|
1Bergman A G,Bogotova E I.Zh Neorg Khim,1964;9:2182 2方建慧,陈念贻,阎立诚,王继扬.见:史启祯,陈佩珩,冉新权,唐宗薰,张逢星主编,第八届全国相图学术会议论文集。西安:西北大学,1995:115 3Zigg D S,Makovsty L E,Tischer R E,Brown F R,Hercules M J.J Phys Chem,1980;84:2898 4Bergman A G,Semenyakova L V.Vkr Khim Zh,1971;37:15 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|