ANALYSIS OF IMPACT BEHAVIOR DURING BALL MILLING
YANG Junyou; ZHANG Tongjun; CUI Kun; HU Zhenhua (Huazhong University of Science and Technology; Wuhan 430074)(Manuscript received 1996-03-18)
Cite this article: 

YANG Junyou; ZHANG Tongjun; CUI Kun; HU Zhenhua (Huazhong University of Science and Technology; Wuhan 430074)(Manuscript received 1996-03-18). ANALYSIS OF IMPACT BEHAVIOR DURING BALL MILLING. Acta Metall Sin, 1997, 33(4): 381-385.

Download:  PDF(379KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By analysing the kinetics of planetary ball milling, the impact behavior of milling ball is investigated, theoretical relationships between the technical parameters of ball milling (RBP= ball to powder ratio,Ω: angular velocity of milling and rb: radius of ball) and the velocity (vb), average free path (S) and impact frequency (f) of milling ball are established in this paper, It shows that vb and f increase with increasing angular velocity of milling; keeping the mass of powders invariable,f increases with increasing RBP, however, vb and S decrease;when mP and RBP are constant, S decreases and f increases with decreasing rb.
Key words:  ball milling      mechanical alloying      average free path     
Received:  18 April 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I4/381

1Koch C C.Cavin O B,Mckamey C G,Scarbrough O J.Appl Phys Lett,1983;43:1017
2杨君友,张同俊,崔 .材料导报,1994;2:11
3Ruusuane P,Heczke O.PB 165108,1993
4木村博,小林信一。粉体粉末冶金,1992;39(1):287
5Davis R M,Mcdermott B,Koch C C. Metall Trans,1988;19A:2867
6Rydin R W.Maurice D R,Courtney T H.Metall Trans,1993;24A:175
7Brun P Le,Froyen L,Dalaey L.Mater Sci Eng,1993;161A:75
8Abdellaoui M,Gaffet E. Acta Metall Mater,1993;43:1087
9Maurice D R,Courtney T H.Metall Transs,1990;21A:289
10钱伟长,叶开源.弹性力学.北京:科学出版社,1980:327
[1] BI Sheng, LI Zechen, SUN Haixia, SONG Baoyong, LIU Zhenyu, XIAO Bolv, MA Zongyi. Microstructure and Mechanical Properties of Carbon Nanotubes-Reinforced 7055Al Composites Fabricated by High-Energy Ball Milling and Powder Metallurgy Processing[J]. 金属学报, 2021, 57(1): 71-81.
[2] Min ZHU, Zhongchen LU, Renzong HU, Liuzhang OUYANG. DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. 金属学报, 2016, 52(10): 1239-1248.
[3] HU Na, XUE Lihong, GU Jian, LI Heping, YAN Youwei. OPTIMIZATION OF GRADING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al13Fe4/Al COM- POSITES IN SITU SYNTHESIZED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2015, 51(2): 216-222.
[4] GU Jian, GU Sasa, XUE Lihong, WU Shusen, YAN Youwei. MICROSTRUCTURE EVOLUTION OF Al-Fe ALLOYS PREPARED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2013, 29(4): 435-442.
[5] WANG Man, ZHOU Zhangjian, YAN Zhigang, YU Pengfei, SUN Hongying. TEM CHARACTERIZATION OF DISPERSOIDS AND MICROSTRUCTURE OF ODS-316 AUSTENITIC STEEL[J]. 金属学报, 2013, 49(2): 153-158.
[6] LU Zheng, LU Chenyang, ZHANG Shouhui, XIE Rui, Liu Chunming. PREPARATION AND CHARACTERIZATION OF NANO-STRUCTURED 14Cr-ODS FERRITIC STEEL[J]. 金属学报, 2012, 48(6): 649-653.
[7] LIU Rongming, YUE Ming, ZHANG Dongtao,Liu Weiqiang, ZHANG Jiuxing. PREPARATION, STRUCTURE AND MAGNETIC PROPERTIES OF SmCo5 NANOPARTICLES AND NANOFLAKES[J]. 金属学报, 2012, 48(4): 475-479.
[8] CHEN Xuebing SHAO ZhongbaoTIAN Yanwen. PREPARATION OF LUMINESCENT MATERIALS BaMoO4:Eu3+ BY HIGH TEMPERATURE BALL MILLING[J]. 金属学报, 2010, 46(7): 862-866.
[9] YANG Shaobin,SHEN Ding,LI Qiang. SYNTHESIS AND ELECTROCHEMICAL PROPERTIES OF Sn0.35-0.5xCo0.35-0.5xZnxC0.30 COMPOSITE[J]. 金属学报, 2010, 46(1): 6-12.
[10] WANG Dong LIU Chunming WANG Changzhen. PREPARATION AND CHARACTERISTICS OF HIGH TEMPERATURE PROTON CONDUCTOR Ba3Ca1.18Nb1.82O9-δ[J]. 金属学报, 2009, 45(3): 345-350.
[11] . MICROWAVE ABSORBING CAPABILITY OF FeSiAlCr NANO-CRYSTALLINE FLAKES[J]. 金属学报, 2006, 42(3): 321-324 .
[12] ZHANG Laichang; SHEN Zhiqi; XU Jian. The Role of Sn Substitution for Si And B to Enhance the Amorphization of Mechanically-Milled Ti50Ni22Cu18Al4Si4B2 Alloy[J]. 金属学报, 2004, 40(9): 981-986 .
[13] ZHANG Xiaoqiang; XU Jian. Formation of W Particles /La55Al25Cu10Ni5Co5 Glassy Alloy Matrix Composites By Mechanical Milling[J]. 金属学报, 2004, 40(6): 647-.
[14] HANG Laichang; SHEN Zhiqi; XU Jian. MECHANICALLY--DRIVEN AMORPHIZATION IN A (Ti, Zr, Hf)--(Cu, Ni, Ag)--Al MULTICOMPONENT ALLOY SYSTEM[J]. 金属学报, 2004, 40(4): 421-428 .
[15] REN Shan; HONG Lan; ZHANG Jinxiu (Department of Physics; Zhongshan University; Guangzhou 510275)LU Manqi; HU Zhuangqi (State Key Lab of RSA; Institute of Metal Research; Shenyang 110015). HYDROGEN INDUCING AMORPHIZATION OF Ti-Fe SYSTEM IN MECHANICAL ALLOYING[J]. 金属学报, 1998, 34(4): 373-377.
No Suggested Reading articles found!