Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (10): 1101-1104    DOI:
Current Issue | Archive | Adv Search |
DETERMINING OF MASS TRANSPORT COEFFICIENT OF PHOSPHORUS IN C-SATURATED MOLTEN IRON
GUO Xingmin;HAN Qiyong (University of Science and Technology Beijing; Beijing 100083) LIU Liu; DING Rong; JIN Zhenjian (Central Iron and Steel Research Institute; Ministry of Melallureical Industry; Beijing 100081)
Cite this article: 

GUO Xingmin;HAN Qiyong (University of Science and Technology Beijing; Beijing 100083) LIU Liu; DING Rong; JIN Zhenjian (Central Iron and Steel Research Institute; Ministry of Melallureical Industry; Beijing 100081). DETERMINING OF MASS TRANSPORT COEFFICIENT OF PHOSPHORUS IN C-SATURATED MOLTEN IRON. Acta Metall Sin, 1997, 33(10): 1101-1104.

Download:  PDF(377KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mass transport coefficient of phosphorus in C-saturated molten iron at 1350℃ had been determined during the dephosphorization of dicalcium ferrite by mechanical stir method. The results are shown as follows: the mass transport process of phosphorus in molten iron was promoted by using mechanical stir, and the mass transpori coefficient of phosphorus, kmρm, was equal to 4.60×10-2g / (cm2. s).
Key words:  dicalcium ferrite      dephosphrization reaction      mass transport coefficient     
Received:  18 October 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1101

1郭兴敏,刘浏,金振坚,宋波,韩其勇.钢铁,1995;(12): 16
2中岛义夫,向政登,深见泰民,孙海平,森谷尚玄,丸桥茂昭.铁上钢,1990;76:1823
3 Scheel R. arch. Eisenhuettenwes, 1974; 45: 751
4潘伟,佐野正道,平泽政广,森一美,铁钢,1988;74:1110
5潘伟,佐野正道,平泽政广,森一美.铁钢,1990;76:552
6 竹林康博,莜畸信也,森克己,川合保治.铁钢,1990;76:1480
No related articles found!
No Suggested Reading articles found!