| DIFFUSION AND SOLUBILIZATION OF HYDROGEN IN Ni-BASE SINGLE CRYSTAL SUPERALLOYS |
| WU Qiuyun; ZHANG Jinghua; SUN Xiukui; HU Zhuangqi(National Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
WU Qiuyun; ZHANG Jinghua; SUN Xiukui; HU Zhuangqi(National Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). DIFFUSION AND SOLUBILIZATION OF HYDROGEN IN Ni-BASE SINGLE CRYSTAL SUPERALLOYS. Acta Metall Sin, 1996, 32(9): 938-942.
|
|
|
Abstract The diffusivity, permeability and solubility of hydrogen in DD8 and Rene'N4 superalloys were measured in the temperature range of 30t-420℃ by using ultrahigh vacuum gas permeation technique. The effect of defects on diffusivity and the reason of exothermic reaction of H-solubilization were analyzed. The results show that, in the testing temperature range, the diffusivity, permeability and solubility of hydrogen in DD8 and Rene'N4 superalloys are all in agreement with Arrhenius relationship, and the presence of voids is not the reason of exothermic reaction of H-solubilization.
|
|
Received: 18 September 1996
|
| 1WalstonWS,BernsteinIM,ThompsonAW.MetallTrans,1992;23A:13132BakerCL,CheneJ,BernsteinIM,WilliamsJC,MetallTrans,1988;19A:733SunXiukui,XuJian,LiYiyi.MaterSciEng,1989;A114:1794施雨湘.焊接学报,1988;9:1955XuJ,SunXK,ChenWX,LiYY.ActaMetallMater,1993;41:14556WuQY,SunXK,XuJ,HuZQ.JNon-CrystSolids,tobepublished7XuJ,SunXK,LiuQQ,ChenWX.MetallMaterTrans,1994;25A:5398WuQY,GaoM,SunXQ,HuZQ.ScrMetallMater,tobepublished9ChristmannK.ZNaturforschTeil,1979;34A:2210JohnsonS,MadixRJ.SurfSci,1981,108:7711McCartyJ,FalconerJ,MadixRJ.JCatal,1973;30:23512PaalZoltan,MenonPG.HydrogenEffectsinCatalysis;FundamentalandPracticalApplicalions.NewYork:MarcelDekkerIne,1988:1813LapujouladeJ,NeilKS.JChemPhys,1972;57:353514LuKE,RyeRR.SurfSci,1974;45:67715褚武杨.氢损伤和滞后断裂.北京:冶金工业出版社,1988:262 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|