Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (6): 637-641    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF COMPOSITION OF B_2O_3-MgO-SiO_2-Al_2O_3-CaO SLAG SYSTEM ON PHYSICAL PROPERTIES OF MELT
CUI Chuanmeng; XU Xiuguang; ZHANG Xianpeng; WANG Kuihan; HAN Weiru (Northeastern University; Shenyang 110006)
Cite this article: 

CUI Chuanmeng; XU Xiuguang; ZHANG Xianpeng; WANG Kuihan; HAN Weiru (Northeastern University; Shenyang 110006). EFFECT OF COMPOSITION OF B_2O_3-MgO-SiO_2-Al_2O_3-CaO SLAG SYSTEM ON PHYSICAL PROPERTIES OF MELT. Acta Metall Sin, 1996, 32(6): 637-641.

Download:  PDF(299KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The viscosity and the transition temperature (when the viscosity of slag changes sharply) of melting boron-magnesium-rich slag system of B_2O_3-MgO-SiO_2-Al_2O_3-CaO, as well as the density and the surface tension, were measured by using the spin-cylinder and double-cylinder continuous methods respectively. The results showed that the viscosity and the transition temperature decrease with the increase in the content of B_2O_3 in slags, and increase with the increase in MgO and basicity in slags when B_2O_3 content is constant. The density and the surface tension of the melt increase with increasing MgO or decreasing SiO_2 in slags. The density changes in the range of (2.5 ± 0.5) t·m~(-3), while the surface tension is in 0.4-0.6 N . m~(-1) .
Key words:  boron-rich slag      viscosity      density      surface tension     
Received:  18 June 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I6/637

1崔传孟,张显鹏,刘素兰.矿冶,1994;3(4):682崔传孟,刘素兰,张显鹏,徐秀光,刘亮,闻玉胜.东北大学学报,1994;15:6233崔传孟,刘素兰,张显鹏,马平,潘翠凤.东北工学院学报,1992;13:5514王文忠,余琨,徐金铎.东北工学院学报,1980;1:335ChouKuochin,HuJianhong.MetallTrans,1991;228:276ErnestML,CarlRR,HowardFM.PhaseDiagramsforCeramicsColumbus:TheAmericanCeramicSociety,1969:1517日本金属学会编,王魁汉,徐秀光译.冶金物理化学.北京:冶金工业出版社,1988:1748陈新民主编.火法冶金过程物理化学.北京:冶金工业出版社,1984:275,281
[1] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[2] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[3] MA Jiankai, LI Junjie, WANG Zhijun, WANG Yujian, WANG Jincheng. Bonding Zone Microstructure and Mechanical Properties of Forging-Additive Hybrid Manufactured Ti-6Al-4V Alloy[J]. 金属学报, 2021, 57(10): 1246-1257.
[4] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[5] Xingpin CHEN,Wenjia LI,Ping REN,Wenquan CAO,Qing LIU. Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels[J]. 金属学报, 2019, 55(8): 951-957.
[6] Yubi GAO, Yutian DING, Jianjun CHEN, Jiayu XU, Yuanjun MA, Dong ZHANG. Evolution of Microstructure and Texture During Cold Deformation of Hot-Extruded GH3625 Alloy[J]. 金属学报, 2019, 55(4): 547-554.
[7] Qingdong XU, Kejian LI, Zhipeng CAI, Yao WU. Effect of Pulsed Magnetic Field on the Microstructure of TC4 Titanium Alloy and Its Mechanism[J]. 金属学报, 2019, 55(4): 489-495.
[8] Zixing WANG,Shuo HUANG,Beijiang ZHANG,Lei WANG,Guangpu ZHAO. Study on Freckle of a High-Alloyed GH4065 Nickel Base Wrought Superalloy[J]. 金属学报, 2019, 55(3): 417-426.
[9] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[10] Ming HE, Xianliang LI, Qingwei WANG, Lianyu WANG, Qiang WANG. Influence of Magnetic Shielding on the Power Loss of Induction Heating Power Supply in the Electro-magnetic Induction Controlled Automated Steel Teeming System[J]. 金属学报, 2019, 55(2): 249-257.
[11] XIONG Jian,WEI Dean,LU Songjiang,KAN Qianhua,KANG Guozheng,ZHANG Xu. A Three-Dimensional Discrete Dislocation Dynamics Simulation on Micropillar Compression of Single Crystal Copper with Dislocation Density Gradient[J]. 金属学报, 2019, 55(11): 1477-1486.
[12] Huiying SHI, Chao YANG, Bailing JIANG, Bei HUANG, Di WANG. Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering[J]. 金属学报, 2018, 54(6): 927-934.
[13] Runzhi QIN, Yanxia DU, Minxu LU, Li OU, Haiming SUN. Study of Interference Parameters Variation Regularity and Corrosion Behavior of X80 Steel in Guangdong Soil Under High Voltage Direct Current Interference[J]. 金属学报, 2018, 54(6): 886-894.
[14] Yachao SUN, Minggang ZHU, Rui HAN, Xiaoning SHI, Nengjun YU, Liwei SONG, Wei LI. Magnetic Viscosity of Anisotropic Rare Earth Permanent Films[J]. 金属学报, 2018, 54(3): 457-462.
[15] Jin WANG, Liming YU, Yuan HUANG, Huijun LI, Yongchang LIU. Effect of Crystal Orientation and He Density on Crack Propagation Behavior of bcc-Fe[J]. 金属学报, 2018, 54(1): 47-54.
No Suggested Reading articles found!