HYDROGEN-INDUCED FAILURE OF OIL-WELL TUBULAR STEEL C90
YU Guanghua; CHENG Yihuan; CHEN Hongxing; NIU Xuejun; QIAO Lijie; CHU Wuyang (University of Science and Technology Beijing; Beijing 100083)(Baoshan Corporation of Iron and Steel; Shanghai 201900)
Cite this article: 

YU Guanghua; CHENG Yihuan; CHEN Hongxing; NIU Xuejun; QIAO Lijie; CHU Wuyang (University of Science and Technology Beijing; Beijing 100083)(Baoshan Corporation of Iron and Steel; Shanghai 201900). HYDROGEN-INDUCED FAILURE OF OIL-WELL TUBULAR STEEL C90. Acta Metall Sin, 1996, 32(6): 617-623.

Download:  PDF(550KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Hydrogen-induced failure properties of three oil-well tubular steels(C90, SM90 and SM95) have been compared. The threshold diffusible hydrogen contents of steel SM90, SM95 and C90 for hydogen blistering are 1 .76, 4.3, and 8.38×10-6, respectively, and the total hydrogen contents 4.24, 6.35 and 10.22 × 10-6 respectively. The threshold stresses of hydrogen-induced fracture corresponding to SM90, SM95 and C90 in NACE solution are σ_(th) /σ_s = 0.64, 0.80 and 0.85, respectively. The threshold stress intensity of hydrogen- induced fracture for C90 decreases with the increase in the diffusible hydrogen content w_o and the experimental result which is consistant with theoretical analysis is as follows: K_(IH) = 46- 1 2. 5lnw_0.
Key words:  steel C90      steel SM90      steel SM95      hydrogen damage      hydrogen-induced delayed failure     
Received:  18 June 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I6/617

1褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社,19882RevieRW,SastriVS,HoeyGR,ShehataMT.Corrosion,1993,49:173陈奇志,褚武扬,肖纪美,金属学报,1994;30:A2844蒋兴钢,褚武扬,肖纪美,中国科学,1994;24A:6685GerbrichWW,In:BernsteinIM,ThompsonAWeds.,HydogeninMetal.MetalsPark:ASM,1970:1156RaviK,RamaswamyV,NamboodhiviTKG.MaterSciEng,1993;A169:111
[1] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[2] WU Yichu;CHANG Xiangrong;TIAN Zhongzhuo;XIAO Jimei University of Science and Technology Beijing. HYDROGEN DAMAGE IN HIGH PURITY IRON[J]. 金属学报, 1992, 28(2): 43-46.
No Suggested Reading articles found!