Acta Metall Sin  1996, Vol. 32 Issue (4): 433-437    DOI:
Current Issue | Archive | Adv Search |
CREEP FRACTURE PROCESS COUPLED WITH CAVITATION IN SiC_p-Al COMPOSITE
WANG Daifeng; LI Geyang; LI Pengxing; WU Renjie(State Key Laboratory for MMCs; Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1995-04-14; in revised form 1995-09-14)
Cite this article: 

WANG Daifeng; LI Geyang; LI Pengxing; WU Renjie(State Key Laboratory for MMCs; Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1995-04-14; in revised form 1995-09-14). CREEP FRACTURE PROCESS COUPLED WITH CAVITATION IN SiC_p-Al COMPOSITE. Acta Metall Sin, 1996, 32(4): 433-437.

Download:  PDF(292KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Creep fractured surface of SiC_p-Al composite was quantitatively analyzed by employing image processing technique and solid mechanics principles, and the effective creep strain was determined. It was found that there is exponential relationship between cavity volume fraction and effective creep strain in the vicinity of fracture surface, which elucidates that the cavity growth during tertiary creep stage was controlled by plastic deformation. The presented testing principle and method could be applied to other plastically deformed materials containing cavities. Correspondent: WANG Daifeng,(Institute of Composite Materials, Shanghai Jiaotong University, Shanghai 200030)
Key words:  SiC_p-Al composite      creep fracture process      cavity growth mechanism     
Received:  18 April 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I4/433

1PhillngJ,RidleyN.ResMech,1988;23:312RajR.ActaMetall,1983;31:293王岱峰.上海交通大学硕士学位论文,19934KashyapBP,MukherjeeAK.ResMech,1986;17:293
No related articles found!
No Suggested Reading articles found!