EFFECT OF MILLING ENERGY ON MECHANICAL ALLOYING OF Mo-Si POWDER MIXTURE
LIU Lin; QIN Yong(Institute of Solid Stale Physics; Chinese Academy of Sciences;Hefei 230031) (Manuscript received 1995-06-27; in revised form 1995-11-27)
Cite this article: 

LIU Lin; QIN Yong(Institute of Solid Stale Physics; Chinese Academy of Sciences;Hefei 230031) (Manuscript received 1995-06-27; in revised form 1995-11-27). EFFECT OF MILLING ENERGY ON MECHANICAL ALLOYING OF Mo-Si POWDER MIXTURE. Acta Metall Sin, 1996, 32(4): 423-428.

Download:  PDF(443KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mechanical alloying of Mo-Si powder mixture with atomic ratio of 1:2 under different milling conditions has been studied by means of X-ray diffractometry (XRD), SEM and TEM. It is found that the higher energy milling favours the formation of stable α-MoSi_2, while the lower energy milling promotes the formation of metastable β-MoSi2. Thermodynamics and kinetics aspects related to the different phase transformations have been discussed. Correspondent: QIN Yong,(senior engineer, Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031)
Key words:  Mo/Si reaction      milling energy      α-MoSi_2      β-MoSi_2     
Received:  18 April 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I4/423

1KochCC,CavinOB,McKamcyCG,ScarbroughJO.ApplPhysLett,1983:43:10172FechtNJ,HanG,FuZ,JohnsonWL.JApplPhys,1990;67:17443EchertJ,SchultzL,UrbanK.ZMetallk,1990;81:8624SchultzL,WeckerJ,HellsternE.JApplPhys,1987;61:38535LiuL,DongYD.NanostructMater,1993;2:4636LiuL,PadellaF,GuoW,MaginiM.ActaMetallMater,1995;43:37557SchwarzRB,SrinivasanSR,PetrovicJJ,MaggioreCJ.MaterSciEng,1992;A155:758MaE,PaganJ,GranfordG,AtzmonMJMaterRes,1993;8.18369MarquardDW.JSocIndApplMath,1963;91:43110MaginiM,CollelaC,GuoW,IasonnaA,MartelliS,PadellaF.IntJMechanochemMechAlloying,1994;1:1411MaginiM.MaterSciFor,1992;88-90:12112BurgioN,IasonnaA,MaginiM,MartelliS,PadellaF.ILNuovoCimento,1991;13D:45913MauriceDR,CourtenyTH.MelallTrans,1990;21A:28914AbdellaouiM,GaffetE.JAlloysCompo,1994;209:35115DolandCM,NemanichRJ.JMaterRes,1990;5:2854
No related articles found!
No Suggested Reading articles found!