| MORPHOLOGY OF SERRATED FLOW OF AI-Li SINGLE CRYSTALS |
| TIAN Baohui; ZHANG Yonggang; CHEN Changqi(Beijing University ofAeronautics and Astronautics; Beijing 100083) (Manuscript received 1 995-05- 1 6; in revised form 1 995-08-25) |
|
Cite this article:
TIAN Baohui; ZHANG Yonggang; CHEN Changqi(Beijing University ofAeronautics and Astronautics; Beijing 100083) (Manuscript received 1 995-05- 1 6; in revised form 1 995-08-25). MORPHOLOGY OF SERRATED FLOW OF AI-Li SINGLE CRYSTALS. Acta Metall Sin, 1996, 32(3): 249-253.
|
|
|
Abstract The serration flow and its morphology of Al-Li single crystal were investigated under different temperatures(T) and strain rates(ε). The critical strain of serration(εc) first increased and then decreased with increasing T or decreasing ε. Temperature and strain rate have some influences on the frequency and amplitude of serration which changed irregularly with deformation. The relations between the type of the serration and the mechanisms for the occurrence of serration, and the changes of frequency and amplitude were obscure in the Al-Li single crystal. Correspondent: TIAN Baohui, Departinent of Materials, Beijing University of Aeronaulics and Astronautics,Beijing 100083
|
|
Received: 18 March 1996
|
| 1KingJE,YouCY,KnottJF.ActaMetall,1981;29:15532SivakesavamO,SahaGG,RaghavaSrinirasaK.MalerSciTechnol,1988;4:5783DelafasseD,LapassetG,KubinLP.ScrMetallMater,1993;29:13794KumarS,PinkE.ScrMetallMater.1995;32:7495PinkE,GrinbergA.MaterSciTechnol,1981;51:16FujitaH,TabataT.ActaMetallMaler,1977;25:7937HuangJC,GrayGT.ScrMetallMaler.1990:26:858BrechetY,EstinY.ScrMetall,1994;31:185 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|