Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (2): 149-153    DOI:
Current Issue | Archive | Adv Search |
STRUCTURAL HEREDITY EFFECT OF REFINEMENT EFFICIENCY FOR AlTiB MASTER ALLOYS
LIU Xiangfa; BIAN Xiufang; LI Hui; MA Jiaji(Shandong University of Technology;Jinan 250014)(Manuscript received 1995-02-17; in revised form 1995-07-05)
Cite this article: 

LIU Xiangfa; BIAN Xiufang; LI Hui; MA Jiaji(Shandong University of Technology;Jinan 250014)(Manuscript received 1995-02-17; in revised form 1995-07-05). STRUCTURAL HEREDITY EFFECT OF REFINEMENT EFFICIENCY FOR AlTiB MASTER ALLOYS. Acta Metall Sin, 1996, 32(2): 149-153.

Download:  PDF(461KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  It has been found by comparative experiments that Al-5Ti-1B master alloys with different structures have different grain refinement efficiency. The microstructure of the master alloys have been characterized using metallograph, SEM and TEM. The effect of structural heredity on grain refinement efficiency is discussed. The experimental results show that the AlTiB master alloy manufactured by rapid solidification method comprises fine TiAl_3 phases and seperate array of boride microparticles, and has the best grain refinement efficiency.(Correspondent LIU Xiangfa, College of Materials Science and Engineering, Shandong University of Technology, Jinan 250014)
Key words:  AlTiB      refinement efficiency      structural heredity effect     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/149

1刘相法,边秀房.铸造,1994;(10):182刘相法,边秀房.铸造,1994;(6):173GuzowskiMM.Metalltrans,1987;184:6034CarverRF.LightMetals,TheMinerals,Metals&MateralsSociety,1990:8455CibulaA.JInstMetals,1949一50;76:3216CrossleyFA,MondolfoLF,JMet,1951;3:11437McCartneyDG.IntMaterRev,1989;34(5):2478KiusalaasR.chemCommun,1986;(1):1
No related articles found!
No Suggested Reading articles found!