Abstract An assembly for performing EMF measurements using a CaF2 single crystal as a solid state electrolyte has been constructed. From the EMF data, the standard Gibbs energies of formation of member oxides in the Sm-Ba-Cu-O system were calculated. It is found that the thermodynamic stability of the complex oxide Sm_(1+x)Ba_(2-x)Cu_3O_y(0≤x≤0.4)decreases with the increase in the solid solubility x.(Correspondent: XING Xianran, associate professor-Department of Physical Chemistry, University of Science and Technology Beijing, Beijing 100083.)
|
|
Received: 18 February 1996
|
| 1RothRS.AdvCeramMater,1987;2:3032AsanoH,YokoyamaY.ModernPhysLettB,1988;2:5833JCPDSCard,6一399,19884QiaoZhiyu,XingXianran,YuanWenxia,WeiSoukun,ChenXiaolong,LiangJinkui,XieShishen.JAlloysCompounds,1993,202:775邢献然.北京科技大学博士论文,19936BarinI,KnackeO,KubachewskiO.Thermochemicalpropertiesofinorganicsubstancesandsupple-ment,Dusseldorf:Springer-Verleg,19777XingXianran,QiaoZhiyu,YuanWenxia,WeiSoukun,ChenXiaolong,RaoGuanghui,LiangJinkui.JMaterSciTech,1994;10:269 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|