SOLIDIFICATION MODEL OF ROD EUTECTIC
PAN Ye; SUN Guoxiong(Southeast University; Nanjing 210018)(Manuscript received 1995-04-24)
Cite this article: 

PAN Ye; SUN Guoxiong(Southeast University; Nanjing 210018)(Manuscript received 1995-04-24). SOLIDIFICATION MODEL OF ROD EUTECTIC. Acta Metall Sin, 1996, 32(2): 120-126.

Download:  PDF(436KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on correspondence between solidification cell and Saffman-Taylor finger, a solidification model of rod eutectic is proposed and used to indicate that the law of phase spacing selection can be expressed by. The effectiveness of the model is experimentally verified by MnSb/Sb eutectic growth. It is found that nf/nf MnSb/Sb and f/nf Si/Al, MnBi/Bi rod eutectics have a nearly same coupling parameter σeff and the similarity of phase spacing selection in microstructure.(Correspondent. PAN Ye, associate professor, Department of Mechanical Engineering, Southeast University,Nanjing 210018)
Key words:  rod eutectic      coupling model      MnSb/Sb growth      phase spacing selection     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/120

1JacksonKA,KuntJD,TransAIME,1966;236:11292MagninP,TrivediR,ActaMetallMater,1991;39:4533SatoT,SayamaY.JCrystGrowth,1974;22:2594FisherDJ,KurzW.ActaMetall,1980;28:7775MagninP,KurzW.ActaMetall1987;35:11196MashaalM,AmarMB,Hakim.VPhyRev,1990;41:44217PelceP,PumirA.JCrystGrowth,1985;73:3378KarmaA.PhysRev,1986;34:43539KarmaA,PelceP,PhysRev,1990;41:674110TrivediR,MagninP,KurzW.ActaMetall1987;35:97111虞觉奇,易文质,陈邦迪,陈宏鉴.二元合金状态图集.上海:上海科学技术出版社,1987:46312HoganLM,SongH.MetallTrans,1987;18A:70713于金,东南大学博士论文,1992:3114NotisMR,ShahDM.IEEETransonMagn,1979,Mag-15:95715刘俊明.物理学报,1992;41:861t
[1] JIAO Yuning;LIU Qingmin;YANG Yuangsheng;GE Yunlong;HU Zhuangqi(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 4 October;1993;in revised form 12 November;1993). EFFECTS OF ELECTROMAGNETIC FLUID FLOW ON Al-Al_2Cu EUTECTIC MORPHOLOGIES[J]. 金属学报, 1994, 30(6): 286-288.
No Suggested Reading articles found!