HYDROGEN EMBRITTLEMENT BEHAVIOUR IN Fe_3Al |
ZHANG Jianmin(Central Iron and Steel Research Institute;Ministry;of Metallurgical Industry;Beijing 100081)ZHANG Ruilin;YU Ruihuang(Jilin University;Changchun 130023)(Manuscript received 1994-08-29;in revised form 1995-02-05) |
|
Cite this article:
ZHANG Jianmin(Central Iron and Steel Research Institute;Ministry;of Metallurgical Industry;Beijing 100081)ZHANG Ruilin;YU Ruihuang(Jilin University;Changchun 130023)(Manuscript received 1994-08-29;in revised form 1995-02-05). HYDROGEN EMBRITTLEMENT BEHAVIOUR IN Fe_3Al. Acta Metall Sin, 1995, 31(7): 300-303.
|
Abstract The effect of hydrogen on the bond structures.bond energy and electron distributions of intermetallic compound Fe3Al is investigated by Empirical Electron Theory of Solids and Molecules.The hydrogen embrittlement in Fe3Al is due to dissolving of hydrogen atoms to change the atomic state of Fe3Al resulting from the sharply reduction of lattice electrons,which cause the decrease of local metallicity,and the formation of severely anisotropic bond structures.At the same time,the hydrogen atoms may occupy the interstitial sites in Fe3Al.Correspondent.ZHANG Jianmin,postdoctoral,(Department of Superalloy,Central Iron and Steel ResearchInstitute,Ministry of Metallurgical Industry,Beijing 100081)
|
Received: 18 July 1995
|
1McKameyCG,DeVanJH.TortorelliPF,SikkaVK.JMaterRes,1991;6:17792殷为民,郭建亭,胡壮麒.材料科学进展,1992;6:2773HaKF,LiuY,AnZZ.MetallTrans,1991;22A:2614TelemanAS,WagnerCNJ,RobertsonWD.ActaMetall.1961;9:2055StoloffNS,LiuCT.Intermetallics,1994:2:756林栋梁.机械工程材料,1994;1:87张瑞林.固体与分子经验电子理论,长春:吉林科学技术出版社,19938张建民.Fe-Al合金的电子理论研究,吉林大学博士学位论文,19949张建民,张瑞林,余瑞璜.科学通报,1995;40:23410张建民,仲增墉,张瑞林,余瑞璜.第八届全国高温合金年会论文,(已接收) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|