| PHENOMENA OF THREE-DIMENSIONAL FLOW AND MIXING IN ARGON-STIRRED LADLES |
| ZHU Miaoyong; SW ADA Ikuo; XIAO Zeqiang (Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Kawasaki 211 Japan)(Manuscript received 1994-03-30; in revised form. 1995-03-13) |
|
Cite this article:
ZHU Miaoyong; SW ADA Ikuo; XIAO Zeqiang (Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Kawasaki 211 Japan)(Manuscript received 1994-03-30; in revised form. 1995-03-13). PHENOMENA OF THREE-DIMENSIONAL FLOW AND MIXING IN ARGON-STIRRED LADLES. Acta Metall Sin, 1995, 31(20): 346-352.
|
|
|
Abstract 3-dimensional fluid flow and mixing characteristics in gas-stirred ladles were studied by using the authors'code. The effects of various operating conditions on fluid patterns and mixing in gas-mstirred ladles were investigated. An empirical relationship for mixing time and an optimum location for the nozzle in the ladle were proposed. The predicted results are in good quantitative agreements with the measured ones. Correspondent: ZHU Miaoyong, postdoctoral, Deportment of Ferrous Metallurgy, Northeastern University.Shenyang 110006
|
|
|
| 1SzekelyJ,WangHJ,KiserKM.TransISIJ,1975;15:2712HsiaoTC,LehnerT,KjellbergB.ScandJMetall,1980;9:1053CastillejosAH,BrimacombeJK.MetallTrans,1989;20:6034JooS,GuthrieRIL,KamalG.SteelmakingProc,1989;72:5175JonesWP.LaunderBE.IntJHeatMassTransfer,1972:15:3016LaunderBE,SpaldingDB.ComputMathApplMechEng,1974;3:2697CastillejosAH,BrimacombeJK.MetallTrans,1987;18:6598PatankarSV.Numericalheattransferandfluidflow.HemisperePubCo,19809朱苗勇.东北大学博士学位论文,199410MietzJ,OetersF.SteelRes.1989.60:38711MietzJ.OetersF.SteelRes,1988:59:5212MaruyamaT,KamishimaN,MizushinaT.JChemEngJpn,1984;17:12013SchwarzMP.LSIJInt.1991;31:947N |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|