Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (18): 255-261    DOI:
Current Issue | Archive | Adv Search |
MODIFIED FORMS FOR SERIES REPRESENTATIONS OF THERMODYNAMIC PROPERTIES OF BINARY SYSTEMS
SU Yi; WANG Zhichang(Northeastern University; Shenyang 110006)
Cite this article: 

SU Yi; WANG Zhichang(Northeastern University; Shenyang 110006). MODIFIED FORMS FOR SERIES REPRESENTATIONS OF THERMODYNAMIC PROPERTIES OF BINARY SYSTEMS. Acta Metall Sin, 1995, 31(18): 255-261.

Download:  PDF(397KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A modified form has been proposed for Margules expansion, Redlich-Kister expansion and Legendre expansion to represent thermodynamic properties of binary systems with stronger convergency and independent characters for the coefficients.
Key words:  thermodynamic properties      binary systems      Margules expansion      Redlich-Kister expansion      Legendre expansion     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I18/255

1WilliamsRO.CALPHAD,1991:15:12WangZC,LuckR,PredelB.CALPHAD,1990;14:2153WangZC,LuckR,PredelB.CALPHAD,1990:14:2354WangZC,LuckR,PredelB,CALPHAD,1993;17:3035KumarKCH.私人通讯,19936WangZC.JChemSocFaradayTransI,1986;82:3757王之昌,中国科学,1986,A(8):8628WangZC.JChemSocFaradayTransI,1987,83:33679WangZC,ZhangXH,ZhouJK.MetallTrans,1992,23B:62310WangZC,TianYW,YuHL,ZhangXH,ZhouJK.MetallTrans,1992,23B66611TianYW,YuHL,WangZC,ZhangXH,ZhouJK.JChemThermodyn,1993,2571112WangZC,TianYW,YuHL,ZhangXH,ZhouJK.MetallMaterTrans,1994,23B.10313BaleCW,PeltonAD.MelallTrans,1974,5232314BaleCW,PeltonAD.CanMetallQ,1975,14.21315PeltonAD,BaleCW.MelallTrans,1986,17A105716HillertM.CALPHAD,1980,4117HultgrenR,DesalPD.HawkinsDT,GleiserM,KellyKK.SeleciedValuesoftheThermodynamicPropertiesofBinaryAlloys,MetalsPark,Ohio:ASM,1973:737,83818HultgrenR,OrrRL,AndersonPA,KellyKK.SelectedValuesoftheThermodynamicPropertiesofMetalsandAlloys,NewYork:Wiley,1963.53
[1] ZHOU Qianli;DU Ting Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. THERMODYNAMICS OF Fe-Nb-Ce LIQUID SOLUTIONS CONTAINING TRACE O, S AND C[J]. 金属学报, 1989, 25(1): 91-95.
No Suggested Reading articles found!