| KINETIC EXPRESSION FOR Al DEGENERATION OF ALUMINIZING LAYER ON STEEL |
| MENG Jilong;LI Hiong;WEI Hingzhao;LI Wenfang;LI Youlin;ZENG Meiqin(South China University of Technology; Guangzhou) |
|
Cite this article:
MENG Jilong;LI Hiong;WEI Hingzhao;LI Wenfang;LI Youlin;ZENG Meiqin(South China University of Technology; Guangzhou). KINETIC EXPRESSION FOR Al DEGENERATION OF ALUMINIZING LAYER ON STEEL. Acta Metall Sin, 1994, 30(19): 327-329.
|
|
|
Abstract Based on Fick's law, the kinetic expression considering the variance of interdiffusion coefficients in Fe-Al-C system with AI concentration was derived for estimating the AI degeneration of aluminized layer on steel undergone high temperature oxidation. The calculated values obtained were in fair agreement with the measured ones by experiments.
|
|
|