| REPASSIVATION POTENTIAL FOR CREVICE CORROSION OF COMMERCIALLY PURE ALUMINUM |
| LIANG Chenghao(Dalian University of Technology)(Manuscript received 23 June;1993;in revised form 23 September;1993) |
|
Cite this article:
LIANG Chenghao(Dalian University of Technology)(Manuscript received 23 June;1993;in revised form 23 September;1993). REPASSIVATION POTENTIAL FOR CREVICE CORROSION OF COMMERCIALLY PURE ALUMINUM. Acta Metall Sin, 1994, 30(16): 165-168.
|
|
|
Abstract The repassivation potential for crevice corrosion(ER) of commercially pure Al was measured successfully using the method developed for stainless steels.The ER is a characteristic value depending on the geometry of the crevice configuration.The ER coincides with that lower limit of critical potential VCREV for crevice corrosion.The results showed that ER of commercially pure Al was less noble than the pitting potential by 100 mV,confirming that crevice corrosion is the more easily occurring type even in commercially pure Al.Correspondent:LIANG Chenghao,associate professor,(Dalian University of Technology,Dalian 116012)
|
|
|
| 1川茂男,久松敬弘.防食技术,1980:29(1):372梁成浩,火时中,谷金香,徐儒庸.太阳能学报,1996:7(3):3223ForoulisZ,A,ThubriarMJ.JElectrochemSOC,1969;116:9064川茂男,张恒,久松敬弘.防食技术,1983;32(3):1495梁成浩,原正,川茂男.防食技术,1988;37(11):6792 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|