Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (14): 77-81    DOI:
Current Issue | Archive | Adv Search |
ROLE OF MULTI-ARC PLATED Ti-N FILM AS A DIFFUSION BARRIER
WANG Jiajun(Tsinghua University; Beijing);YE Ruizeng(University of Science and Technology Beijing);SUN Yufang(General Research institute for Nonferrous Metals;Beijing)(Manuscript received 27 July;1993;in revised form 6 September 1993)
Cite this article: 

WANG Jiajun(Tsinghua University; Beijing);YE Ruizeng(University of Science and Technology Beijing);SUN Yufang(General Research institute for Nonferrous Metals;Beijing)(Manuscript received 27 July;1993;in revised form 6 September 1993). ROLE OF MULTI-ARC PLATED Ti-N FILM AS A DIFFUSION BARRIER. Acta Metall Sin, 1994, 30(14): 77-81.

Download:  PDF(374KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Several multi-layer coatings have been designed so as to assess the diffusion barriering ability against Al,Ni,Co,etc.as well as the high temperature stability of the multi-arc plated Ti-N film after being aged at 1000 and 1100℃ for a long time.The results show that,up to 1000℃,Ti-N film is of good stability;it can prevent effectively Al from diffusing towards matrix,and slow down the rate of diffusion of Ni,Co from CoCrAlTaY to matrix.Above 1100℃,the morphology of Ti-N film changes from thin foil to particles.Apparently the particle-shaped Ti-N can not prevent Ni,Co from the inter-diffusing between matrix and CoCrAlTaY coating.
Key words:  overlaying coating      diffusion-barrier coating      inter diffusion effect      Ti-N coating     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I14/77

1GowardG.Trans ASM,1967;60:2282HsuLL.SurfCoatTechnol,1987;32:13RestallJE.In:Meethan G W ed.,TheDevelopmentofGasTurbineMaterials,London:AppliedScience.1981:2804王家军,叶锐曾,于文秀,孙庆标,马跃发,陈仁治.北京科技大学学报,1991;13:5795CoadJP,RickerbyD S,OberlanderN.MaterSciEng,1985;74:936Young SG,ZellarsGR.ThinSolidFilms,1978;53:2417王家军.北京科技大学硕士学位论文,1990J
No related articles found!
No Suggested Reading articles found!