Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (11): 491-501    DOI:
Current Issue | Archive | Adv Search |
SYMPATHETIC-LEDGEWISE MECHANISM OF BAINITIC TRANSFORMATION
FANG Hongsheng;WANG Jiajun(Tsinghua University; Beijing)(Manuscript received 20 July; 1994)
Cite this article: 

FANG Hongsheng;WANG Jiajun(Tsinghua University; Beijing)(Manuscript received 20 July; 1994). SYMPATHETIC-LEDGEWISE MECHANISM OF BAINITIC TRANSFORMATION. Acta Metall Sin, 1994, 30(11): 491-501.

Download:  PDF(891KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The main problems encountered by shear and diffusion controlled ledgewise mechanisms of bainitic transformation have been reviewed. Based on the ledgewise growth theory, a sympathetic-ledgewise mechanism and its transformation model describing bainitic formation in both steels and non-ferrous alloys have been presented. Correspondent: WANG Jiajun,Depantment of Materials Science, Tsinghua Univesity, Beijing 100084)
Key words:  bainitic transformation      transformation mechanism      transformation model      sympathetic-ledgewise mechanism     
Received:  18 November 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I11/491

1HehemannRF,KinsmanKR,AaronsonHI.MetallTrans,1972;3A:10772AaronsonH I,ReynoldsWTJr,ShifletGJ,SpanosG.MetallTrans,1990;21A:13433SpeichGR.In:ZackayVF,AaronsonHIeds.,DecompositionAustenitebyDiffusionalProcesses,NY:IntersclencePublishers,1962:3534BhadeshiaHKDH,WaughAR,ActaMetall,1982;30:7755UnikrishnanM.J MaterSci,1978;13:14016 ClarkHM,WaymanCM,In:AaronsonHIed.,PhaseTransformations.MetalsPark,OH:ASM1970:597 SrinivasanGR,WaymanCM.ActaMetall,1968,16:6098WastonJD,McDougallPG.ActaMetall,1973;21:9619AaronsonHI.In:ZackayVF,AaronsonHIeds.,DecompositionAustenitebyDiffusionalPro-cesses,NY:IntersciencePublishers,1962:38710 Bhadeshia H KDH,EdmondsDV.ActaMetall,1980;28:110311 BhbadeshiaHKDH,ChristianJW.MetallTrans.1990;21A:76712FangHS,WangJJ,ZhengYK.MetallTrans,1994;25A,inpublishing13FangHS,WangJJ,ZhengYK,In:TamuraIed.,Heat&Surfac’92,Tokyol:JpnTechInformServPubl,1992:57914方鸿生,王家军,郑燕康,杨志刚.金属学报,1993;29:A44515OblackJM,HehemannRF.Tronsformations&HardenabilityinSteels,AnnArbor,MI:ClimaxMolybdenumCompany,1967:1516HehemannRF.In:AaronsonHIed.,PhaseTronsformations,MetalsPark,OH,ASM,1970:39717PickeringFB.Transformations&HardenabilityinSteels,AnnArbor,MI:ClimaxMolybdenumCompany,1967:10918ChristianJW.In:ZackayVF,AaronsonHIeds.,DecompositionAusteniteby DiffusionalPuocesses,NY:IntersciencePublishers,1962:37119ChristianJW.TheMechanismofPhaseTransformationsinCrystallineSolids,London:InstMetalls,1969:12920EichenE,AaronsonHI,PoundGM,TrivediR.ActaMetall,1964;12:129821方鸿生,李春明,王家军.金属学报,1993;29:A38322方鸿生,白秉哲.金属学报,1986;22:A28323HabrakenLJ,EconomopoulosM.Transformations&HardenabilityinSteels.AnnArbor,MI:ClimaxMolybdenumCompany,1967:6924NilanTG.Transformations&HardenabilityinSteels, Ann Arbor,MI:ClimaxMolybdenumCom-pany,1967:5725KinsmanKR,AaronsonHI.MetallTrans,1970;1A:148526FangHS,WangJJ,LiCM.PacificRimConferenceontheRolesofShear&DiffusionintheFor-mationofPlate-ShapedTransformationProducts,Hawaii,USA:1992;1527ChristianJW,EdmondsDV.PhaseTransformations.inFerrousalloy,Warrendale,PA:TMS,1984;29328王家军,清华大学博士学位论文,199329王家军,方鸿生,杨志刚,李春明.金属热处理学报,1994;15(2):1330方鸿生,王家军,杨志刚,李春明,邓旭蕊,郑燕康.自然科学进展,1993:3:52531AaronsonHI,WellC.TransAIME,1956;206:121632WangJJ,FangHS,YangZG,ZhengYK.MaterChar,1994,inpublishing33王家军,方鸿生,郑燕康,严隽珏.兵器材料科学与工程,1993;16(4):334严隽珏,方鸿生,王家军.科学通报,1994,39:11435FangHS,WangJJ,ZhengYK.Heat&Surface’94,France,Seine,199436StreetJA,JInstMetals,1959;88:38137 MenonESK,AaronsonHI.AclaMetall,1987;35:549?
[1] WAN Xiangliang, HU Feng, CHENG Lin, HUANG Gang, ZHANG Guohong, WU Kaiming. Influence of Two-Step Bainite Transformation on Toughness in Medium-Carbon Micro/Nano-Structured Steel[J]. 金属学报, 2019, 55(12): 1503-1511.
[2] WANG Changjun, SUN Xinjun, YONG Qilong, LI Zhaodong, ZHANG Xi, JIANG Lu. EFFECT OF BAINITIC TRANSFORMATION TEMPERATURE ON THE MICROSTRUCTURES AND MECHANICAL PROPERTIES OF THE HOT ROLLED TRIP STEEL CONTAINING Ti AND Mo AND ITS PRECIPITATION CHARACTERISTICS[J]. 金属学报, 2013, 29(4): 399-407.
[3] FENG Chun. The lower bainitic carbides are precipitated from austenite[J]. 金属学报, 2007, 43(6): 583-588 .
[4] WANG Zhenqing; ZHOU Bo; LIANG Wenyan. The constitutive relationship of shape memory alloy[J]. 金属学报, 2007, 43(11): 1211-1220 .
[5] XU Zuyao T. Y. Hsu. Effect of Stress on Bainitic Transformation in Steel[J]. 金属学报, 2004, 40(2): 113-119 .
[6] J.W.Christian FRS(Department of Materials; Oxford University; Parks Road; Oxford OX1 3PH; UK). INTERFACES IN PHASE TRANSFORMATIONS[J]. 金属学报, 1997, 33(2): 150-156.
[7] FANG Hongsheng;LI Chunming;WANG Jiajun Tsinghua University; Beijing100084. INITIAL α_1 PLATES AND THREE-DIMENSIONAL LEDGES OF BAINITE IN A Cu-Zn-Al ALLOY[J]. 金属学报, 1993, 29(9): 1-5.
[8] XU Zuyao;ZHOU Xiaowang T. Y. Hsu; Shanghai Jiaotong University Correspondent professor; Department of Materials Science; Shanghai Jiaotong University; Shanghai 200030. THERMODYNAMICS OF BAINITIC TRANSFORMATION IN A Cu-24at.-%Al ALL0Y[J]. 金属学报, 1992, 28(6): 26-28.
[9] DONG Jianxin;CHEN Fumin;CHEN Jinming;LIU Wenxi Tianjin University. MICROSTRUCTURE AND REVERSE SHAPE MEMORY EFFECT IN A Cu-Zn-Al ALLOY[J]. 金属学报, 1990, 26(6): 81-83.
[10] CAO Renhuan;MA Hongti Northest University of Technology;ShenyangYAN Zhenqi Professor;Depariment of Metallic Materials;Northeast University of Technology;Wenhua Rood;Shenyang. BAINITIC TRANSFORMATION IN LOW CARBON Mn-Nb-V AND Mn-Mo-Nb-V STEELS[J]. 金属学报, 1988, 24(2): 135-138.