| SLIP BANDS OF PRESTRAINED AND CYCLED Cu AND Cu-Zn ALLOY |
| CHAI Huifen;RUAN Zheng;FAN Quncheng (Xi'an Jiaotong University)(Manuscript received 7 December; 1993; in revised form 10 June; 1994) |
|
Cite this article:
CHAI Huifen;RUAN Zheng;FAN Quncheng (Xi'an Jiaotong University)(Manuscript received 7 December; 1993; in revised form 10 June; 1994). SLIP BANDS OF PRESTRAINED AND CYCLED Cu AND Cu-Zn ALLOY. Acta Metall Sin, 1994, 30(11): 502-506.
|
|
|
Abstract The mopohology of slip bands for materials with two different slip modes: pure Cu and Cu-Zn alloy after prestraining and cyclic softening has been observed. Both of their double cross slip bands are rather different, and ones in Cu-Zn alloy is corresponding to the dynamic strain aging. Two kinds of slip bands contrast are shown in the cyclic softened Cu-Zn alloy, but mainly the stationary slip bands appeare in pure Cu. These may indicate that the way to accommodate the cyclic strain is different. According to the feature of slip bands,the mechanical behaviour of softening for the two materials has been explained. Correspondent: CHAI Huifen,(professor, Xi'an Jiaotong University, Xi'an 710049)
|
|
Received: 18 November 1994
|
| 1HallEO.YieldPointPhenomenainMetalsandAlloys.NewYork:PlenumPress,1970:2012HongSI,LairdC.ActaMetall,1990;38:20853MughrabiH.Proc 5thIntConfontheStrengthofMetalsandAlloys,OxfordPergamon,1980:16154LairdC.In:Nabarro F R N ed.,DislocationsinSolids,Vol.6,North—HollandAmsterdam,1983:.575柴惠芬,阮征,范群成,金属学报,1993;29:A153 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|