Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (1): 7-10    DOI:
Current Issue | Archive | Adv Search |
A NEWLY DISCOVERED DIFFUSION MECHANISM IN SOLIDS──COMPLEX DIFFUSION MECHANISM
YU Zongsen;CHEN Ning(University of Science and Technology Beijing)(Manuscript received 21 June;1993)
Cite this article: 

YU Zongsen;CHEN Ning(University of Science and Technology Beijing)(Manuscript received 21 June;1993). A NEWLY DISCOVERED DIFFUSION MECHANISM IN SOLIDS──COMPLEX DIFFUSION MECHANISM. Acta Metall Sin, 1994, 30(1): 7-10.

Download:  PDF(306KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Substitutional solute atoms are believed to difuse by means of solute atom-vacancy complexes.This mechanism could be used to explain some phenomena very well such as:the rule for occurring of non-equilibrium segregation,the anomalously fast diffusion phenomena of solute atoms,the boron's fast diffusion and non-equilibrium segregation of grain-boundary in γ-Fe,the segregation of solute atoms in vacancy-pits on aluminium surface and the precipitation of silicon in the grain-boundary of aluminium.Correspondent:YU Zongsen,professor,(Department of Materials Physics,Universiy of Science and Technology Beijing,Beijing,100083)
Key words:  diffusion mechanism      vacancy.solute atom      non-equilibrium segregation     
Received:  18 January 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I1/7

1ShewmonPG.DiffusioninSolids.NewYork:McGraw-Hill,1990;1132AustKT,HannemanRE,NiessenP,WestbrookJH.ActaMetall1968:16:2913KarlssonLetal.ActaMetall,1988;32:14AnthonyTR.ActaMetall,1970:18:3075余宗森,陈宁.中国科学1992;A10:11146余宗森,陈宁.金属学报,1992;28:A1047陈宁,余宗森,金属学报,待发表8陈宁,余宗森.已投科学通报9陈宁,余宗森.金属学报,1992;28:B39510FaulknerRG,HopkinsTC.X-raySpectra,1977;6:73.11CaiWP.JMatSci,1991;26:381312WarburtonWK,TurnbullD.In:NowickAS,BurtonJJeds.,DiffusioninSolids,NewYork:AcademicPress,1975:17113NakamuraY,NakajimaH,IshiokaS,KoiwaMActaMetall,1988;36:2787.14McLellanRB,KoC,BrotzenFR.ActaMetallMaler.1990;38:2161.15陈宁,余宗森.北京科技大学学报,1992;14:57716郭世宝.北京科技大学硕士论文,1993.17陈宁,余宗森,北京科技大学学报,1994;16:209p
[1] SUN Zhengyang, YANG Chao, LIU Wenbo. Phase Field Simulations of the Sintering Process of UO2[J]. 金属学报, 2020, 56(9): 1295-1303.
[2] CHEN Ning; YU Zongsen (University of Science and Technology Beijing). NON-EQUILIBRIUM SEGREGATION OF Si ON Al-0.35wt-%Si ALLOY SURFACE[J]. 金属学报, 1992, 28(9): 63-66.
[3] ZHANG Lixin;NInG Hua;ZHOU Jing;LI Liguang Laboratory of Corrosion Science; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang Institute of Metal Research; Academia Sinica; Shenyang Correspondent professor; Institute of corrosion and protection of Metals; Academia Sinica; Shenyang 110015).. EFFECT OF NON-EQUILIBRIUM SEGREGATION OF P ON ORIENTATION VARIATION IN COLD ROLLED Fe-P ALLOY[J]. 金属学报, 1992, 28(5): 32-39.
[4] YU Zongsen;CHEN Ning University of Science and Technology Beijing. MECHANISM FOR DIFFUSION OF BORON IN γ-Fe[J]. 金属学报, 1992, 28(3): 10-14.
[5] CHU Youyi;ZHANG Sanhong;HE Xinlai;KE Jun T. Ko Beijing University of Science and Technology. MECHANISM OF NON-EQUILIBRIUM SEGREGATION OF SOLUTE TO GRAIN BOUNDARIES[J]. 金属学报, 1989, 25(4): 41-47.
[6] GAO Qiaojun;T. T. TSONG Beijing University Pennsylvania State University U. S. A. OBSERVATION OF EPITAXIAL OVERLAYER OF METALS AT ATOMIC LEVEL[J]. 金属学报, 1989, 25(1): 1-6.
No Suggested Reading articles found!