SURFACE ALLOYING BY GLOW-DISCHARGE PLASMA WITH ARC SOURCE
PAN Junde;FAN Benhui;LI Chengming;HE Qi;ZHENG Weineng;XU Zhong Taiyuan University of Technology
Cite this article: 

PAN Junde;FAN Benhui;LI Chengming;HE Qi;ZHENG Weineng;XU Zhong Taiyuan University of Technology. SURFACE ALLOYING BY GLOW-DISCHARGE PLASMA WITH ARC SOURCE. Acta Metall Sin, 1993, 29(9): 88-91.

Download:  PDF(651KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Investigation was carried out of titanizing the plain steel by technique ofglow-discharge plasma with arc source. Microstructure, Ti distribution and phases occurredin the infiltration layer and their related processing parameters were examined and discussed.
Key words:  glow-discharge      arc-discharge      surface alloying      cold cathode arc source     
Received:  18 September 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I9/88

1 潘俊德,范本惠,徐重,李成明,韩晋宏,郑维能.CN Pat,90103841. 5,1990
2 Xu Zhong.USA Pat,4520268,1985
3 徐重,王振民,古凤英,范本惠,肖丽华,赵晋香.金属热处理学报,1982;(1) :71
4 张石权.真空,1988;(1) :7
5 王福珍,闻立时.表面沉积技术.北京:机械工业出版社,1989:31
[1] WEI Xiangfei, ZHANG Pingze, WEI Dongbo, CHEN Xiaohu, WANG Qiong, WANG Ruonan. FRICTION AND WEAR PROPERTIES OF SURFACE PLASMA Cr-W ALLOYING LAYER OFγ-TiAl ALLOY[J]. 金属学报, 2013, 49(11): 1406-1410.
[2] HE Xiuli; WANG Huaming (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)ZHENG Qiguang; XU Desheng (State Key Laboratory of Laser Technology; Huazhong University of Science and Technology; Wuhan 430074)Correspondent: WANG Huaming; professor Tel: (010)62017251-7034(O); (010)62013322-5294(H);Fax: (010)62015920; E-mail: Wanghm@mailcity.com. LASER SURFACE ALLOYING OF TiAl INTERMETALLICS WITH CARBON[J]. 金属学报, 1998, 34(9): 983-986.
[3] HE Qi; BIAN Jie; ZHEN Weineng;PAN Junde; FAN Benhui (Taiyuan University of Technology;Taiyuan 030024)(Manuscript received 1996-01-26; in revised form 1996-04-06). MICROSTRUCTURES OF NICKEL-CHROMIZING LAYER ON STEELS BY GLOW-DISCHARGE ION ALLOYING[J]. 金属学报, 1997, 33(4): 406-412.
[4] WANC Zheng;ZHANG Yongsheng Zhengzhou Institute of Technology. INFLUENCE OF Ni-P ELECTROLESS PLATING ON STRESS CORROSION CRACKING OF 304 STEEL[J]. 金属学报, 1991, 27(2): 129-134.
No Suggested Reading articles found!