PREPARATION OF B-N FILMS BY ION BEAM ASSISTED DEPOSITION
JIANG Hai;TAO Kun;LI Hengde Tsinghua University. Beijing lecturer;Department of Materials Science and Engineering;Tsinghua University; Beijing 100084
Cite this article: 

JIANG Hai;TAO Kun;LI Hengde Tsinghua University. Beijing lecturer;Department of Materials Science and Engineering;Tsinghua University; Beijing 100084. PREPARATION OF B-N FILMS BY ION BEAM ASSISTED DEPOSITION. Acta Metall Sin, 1993, 29(4): 77-80.

Download:  PDF(430KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  BN films, synthesized by ion beam assisted deposition, were analysed by RBS,AES, IR spectra and TEM. Formation of c-BN phase was shown not only by IR spectra atabsorption peak of 1100 cm~(-1), but also by electron diffraction pattern. The results of AESdemonstrate an effect of N~+ implantation near the film surface. The deposited films consist ofthree layers, i.e., ion implantation layer, film layer and mixed intermediate layer, according tothe difference of concentration. The micro-Knoop hardess of the film is 25-35 GPa.
Key words:  ion beam assisted deposition      BN film     
Received:  18 April 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I4/77

1 Satou M, Yamaguchi K, Andoh Y, Suzuki Y, Matsuda K, Fujinoto F. Nucl Instrum Methods Phys Res. 1985; B7/Tetreault T G, Hirvonen J K, 8: 910
2 Halverson W D, Tetreault T G, Hirvonen J K. Mater Sci Forum, 1990; 54/55: 71
3 Chu W K, Mayer J W, Nicolet M A. Backscattering spectrometry. Newyork: Academic Press, 1978
4 Verinaud F, Weissmantel E, Grenier I, Celerier A, Machet J, Weissmantel S. Thin Solid Films, 1992: 209: 59
5 Sainty W G, Martin P J, Netterfield R P, Mckenzie D R, Cockayne D J H, Dwarte D M. J Appl Phys, 1988; 64: 3980
[1] ZHU Hong; LIU Xianghuai; REN Congxin; CHEN Guoliang; ZOU Shichang (Ion Beam Lahoratory Shanghai Institute of Metallurgy; Chinese Academy of Sciences;Shanghai 200050). STRUCTURE AND PROPERTIES OF DIAMOND LIKE CARBON FILMS BY LOW ENERGY ION BEAM ASSISTED DEPOSITION USING A SINGLE ION SOURCE[J]. 金属学报, 1995, 31(15): 139-144.
[2] LIU Hanwei;CHEN Yuanru (Southwest Jiaotong University; Chengdu)ZHANG Xushou (Laboratory of Solid Lubrication; Lanzhou institute of Chemical Physics;Chinese Academy of Sciences; Lanzhou). TRIBOLOGICAL PROPERTIES OF TiN FILM BY ION BEAM ASSISTED DEPOSITION[J]. 金属学报, 1994, 30(19): 323-326.
[3] JIANG Hai; WU Qinglan; TAO kun; LI Hengde(Tsinghua University; Beijing). FORMATION OF IRON NITRIDE FILMS BY ION BEAM ASSISTED DEPOSITION[J]. 金属学报, 1994, 30(18): 273-276.
No Suggested Reading articles found!