| CREEP-FATIGUE BEHAVIOUR OF A Ni-BASE SINGLE CRYSTAL ALLOY DD3 AND ITS LIFE PREDICTION |
| SU Hansheng;WU Zhongtang Beijing Institute of Aeronautical Materials |
|
Cite this article:
SU Hansheng;WU Zhongtang Beijing Institute of Aeronautical Materials. CREEP-FATIGUE BEHAVIOUR OF A Ni-BASE SINGLE CRYSTAL ALLOY DD3 AND ITS LIFE PREDICTION. Acta Metall Sin, 1993, 29(1): 25-32.
|
|
|
Abstract Creep-fatigue behaviour of a Ni-base single crystal alloy DD3 under condi-tion of tension-tension stress was investigated from some concept about strain range parti-tioning (SRP) and strain energy partitioning (SEP). Study of effect of hold time and its quan-titative computation was also made. Using numerical method of SEP (SEP-NCM), creep-fa-tigue life prediction under condition of tension-tension strees was performed.
|
|
Received: 18 January 1993
|
1 Miner R V, Gayda J, Hebsur M G. ASTM STP 942. 1988; 371 2 Gabb T P, Welsch G, Miner R V, Gayda J. Mater Sci Eng. 1989: A108: 189 3 Duan Z, He J, Ning Y, Dong Z. ASTM STP 942, 1988: 1133 4 Hoffelner W, Melton K N, Wuethrich C. Fatigue Eng Mater Struct, 1983; 6: 77 5 Draprel J M. AD/A059900, 1978, Al--9----Al--43 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|