Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (8): 49-54    DOI:
Current Issue | Archive | Adv Search |
PHASE DIAGRAM OF TERNARY SYSTEM PrCl_3-SrCl_2-CaCl_2
ZHENG Chaogui; BAO Chenglin (Peking University; Beijing); QIAO Zhiyu(University of Science and Technology Beijing); YE Yupu(Peking University; Beijing).
Cite this article: 

ZHENG Chaogui; BAO Chenglin (Peking University; Beijing); QIAO Zhiyu(University of Science and Technology Beijing); YE Yupu(Peking University; Beijing).. PHASE DIAGRAM OF TERNARY SYSTEM PrCl_3-SrCl_2-CaCl_2. Acta Metall Sin, 1992, 28(8): 49-54.

Download:  PDF(501KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Five fields corresponding to the primary crystallization of PrCl_3, Sr_3PrCl_9, α(SrCl_2, CaCl_2),α_1(CaCl2, SrCl_2) and β_2(SrC12, CaCl_2) respectively, six univariant lines related to the secondary crystallization, one ternary eutectic (48.0 wt-%PrCl_3, 23.5 wt-% SrCl_2; 590℃) and ternary peritectic point (45.5 wt-%PrCl_3, 24.5 wt-% SrCl_2; 614℃ ) were determined by DTA. Attempts were also made to explore the rule governing the alteration in the phase diagram containing rare earth chloride, formation of compound and its stability by means of the theory of polarization and counter-polarization.
Key words:  PrCl_3      PrCl_3-SrCl_2-CaCl_2      phase diagram      phase diagram rule     
Received:  18 August 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I8/49

1 #12
2 #12
3 Sandonnini C. Gazz Chim Ital. 1914; 44(1) : 335
4 郑朝贵,叶于浦.高等学校化学学报,1988;9:423
5 郑朝贵,叶于浦.第5届全国相图学术会议论文集,1988
6 Blachnik R, Alberts G. Z Anorg Chem, 1985; 522:207
7 郑朝贵,张亚钢,陈集林,叶于浦.北京大学学报(自然科学版),1987;(6) :72
8 Kurodo T. Chem Abstract, 1958; 52: 8795p
9 柴良,郑朝贵,叶于浦.中国稀土学报,1990;8(1) :92
10 郑朝贵,刘红平,乔芝郁,叶于浦.金属学报,1990;26:B68
11 Zheng Chaogui, Jin Jun, Chen Jilin, Ye Yupu. Kexue Tongbao, 1989; 34(14) : 1230
12 #12
13 Shannon R D. Acta Crystallogr, 1976; A32:751
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[3] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[4] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[5] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[6] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[7] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[8] YU Jin (Shenyang Polytechnic University; Shenyang 110023) YU Yongli; WANG Zhichang (Northeastern University; Shenyang 110006)(Manuscript received 1996-04-03). MUTUAL SEPARATION OF RARE EARTH CHLORIDE MIXTURES USING A DRY PROCESS[J]. 金属学报, 1997, 33(4): 391-394.
[9] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[10] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[11] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[12] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[13] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
[14] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[15] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
No Suggested Reading articles found!