FATIGUE CRACK PROPAGATION IN Al-Li ALLOY 8090
WANG Zhongguang;ZHANG Yun;HU Zhuangqi;HE Shiyu;LI Qingjian State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang Harbin Institute of Technology; Correspendent profersor; Insitute of Research; Acodemia Sinica; Sheyang 110015
Cite this article: 

WANG Zhongguang;ZHANG Yun;HU Zhuangqi;HE Shiyu;LI Qingjian State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang Harbin Institute of Technology; Correspendent profersor; Insitute of Research; Acodemia Sinica; Sheyang 110015. FATIGUE CRACK PROPAGATION IN Al-Li ALLOY 8090. Acta Metall Sin, 1992, 28(5): 44-50.

Download:  PDF(2091KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fatigue crack growth rates of 8090 type Al-Li alloy in air were found to bestrongly dependent upon the aging conditions. The naturally aged and underaged specimensshowed the highest resistance to the fatigue crack propagation. The fatigue crack growth re-sistance of the overaged specimen is the lowest and that of the peakaged specimen in between.As compared to air, 3.5%NaCl solution did not change the effect of aging conditions on thefatigue crack growth, but caused a decrease of the resistance to the fatigue crack growth un-der the same aging condition. Both short cracks from notch and physically short cracksshowed much higher rates of fatigue crack propagation in comparison with long cracks underthe same aging condition and stress intensity level. The growth behavior of the short crackdepends on its type. The growth rate of short crack from notch decreases first to a minimumand then increases with increasing AK. However, the physically short crack grows at aprogressively increasing rate. The effects of aging conditions were explained in terms of theslip planarity of dislocations and the cyclic slip reversibility. The observed short crack behav-ior was considered to be dependent on the crack closure and the local plasticity near the crack
Key words:  Al-Li alloy      short and long fatigue crack      closure effect      slip planarity     
Received:  18 May 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I5/44

1 Jata K V, Starke E A Jr., Metall. Trans., 1986; 17A: 1011
2 Venkateswara Rao K T, Yu W, Ritchie R O. Metall Trans, 1988; 19A: 549
3 Venkateswara Rao K T, Yu W, Ritchie R O. Metall Trans, l988; 19A: 563
4 陈铮.航空学报,1990;11(8) :B369
5 Nicholls D J, Martin J W. Fatigue Fract Eng Mater Struct, 1990; 13: 83
6 Haddleton F L, Murphy S, Griffin T J. J Phys Colloq, 1987; 48 (9) : 809
7 Peters M, Bachmann V, Welpmann K. J Phys Colloq, 1987; 48 (9) : 785
8 HE S Y, Li QJ, Feng X Z, Wang Z G, Zhang Y. Chin J Met Sci Technol, to be published

9 Allen R J, Booth G S, Jutla T. Fatigue Fract Eng Mater Struct, 1988; 11: 45
10 李清健.哈尔滨工业大学硕士学位论文,1991
11 Ritchie R O, Yu W. In: Ritchie R O, Landford J eds., Small Fatigue Cracks, AIME, 1986: 167--189
12 Guiu F, Stevens R N. Fatigue Fract Eng Mater Struct, 1990; 13: 625
13 Miller K J. Fatigue Fract Eng Mater Struct, 1987; 10: 75-
[1] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[2] LI Shiju, LI Yang, CHEN Jianqiang, LI Zhonghao, XU Guangming, LI Yong, WANG Zhaodong, WANG Guodong. Segregation Behavior, Microstructure and Properties of 2099Al-Li Alloy Produced by Twin-Roll Casting Underthe Action of Electromagnetic Oscillation Field[J]. 金属学报, 2020, 56(6): 831-839.
[3] Chao CAI,Yang LI,Jinfeng LI,Zhao ZHANG,Jianqing ZHANG. Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet[J]. 金属学报, 2019, 55(8): 958-966.
[4] Xu LI,Qingbo YANG,Xiangze FAN,Yonglin GUO,Lin LIN,Zhiqing ZHANG. Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy[J]. 金属学报, 2019, 55(6): 709-719.
[5] Jinfeng LI,Danyang LIU,Ziqiao ZHENG,Yonglai CHEN,Xuhu ZHANG. EFFECT OF Er MICRO-ALLOYING ON MECHANICAL PROPERTIES AND MICROSTRUCTURES OF 2055 Al-Li ALLOY[J]. 金属学报, 2016, 52(7): 821-830.
[6] Xianfeng ZHANG,Guoai LI,Zheng LU,Juan YU,Min HAO. EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY[J]. 金属学报, 2016, 52(12): 1497-1502.
[7] LIU Fenjun, FU Li, ZHANG Wenyuan, MENG Qiang, DONG Chunlin, LUAN Guohong. INTERFACE STRUCTURE AND MECHANICAL PRO-PERTIES OF FRICTION STIR WELDING JOINT OF 2099-T83/2060-T8 DISSIMILAR Al-Li ALLOYS[J]. 金属学报, 2015, 51(3): 281-288.
[8] WANG Dong DONG Chunlin XIAO Bolv GAO Cong HE Miao LUAN Guohong MA Zongyi. EFFECT OF WELDING PARAMETERS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED AlCuLi ALLOY JOINTS[J]. 金属学报, 2012, 48(9): 1109-1115.
[9] SU Jingxin; ZHANG Zhao; CAO Fahe; ZHANG Jianqing; CAO Chunan. EXFOLIATION CORROSION BEHAVIOR OF T6 TREATED 2090 Al-Li ALLOY IN EXCO SOLUTION AND EIS DURING EXFOLIATION CORROSION EVOLUTION[J]. 金属学报, 2005, 41(9): 974-978 .
[10] WU Ximao;Al Suhua;ZHANG Yun;WANG Zhonmang;HAN Xinglin (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Shenyang Polytechnic University. Shenyang 110023). THE LOW CYCLE FATIGUE BEHAVIOUR FOR 8090 Al-Li ALLOYS[J]. 金属学报, 1997, 33(7): 702-708.
[11] Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083). INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS[J]. 金属学报, 1997, 33(6): 577-582.
[12] LIN Zhaoqi;ZHAO Gang; LI Hongxiao; RU Hongqiang; LIU Chunming (Northeastern University; Shenyang 110006). EFFECT OF HYDROGEN CONTENT ON STRUCTURE AND PROPERTIES IN 2091-T6 Al-Li ALLOY SHEET[J]. 金属学报, 1997, 33(10): 1047-1052.
[13] PENG Delin; MIN Guanghui; AN Geying; LIU Hongbo (Harbin Institute of Technology; Harbin 150001). DIRECTIONAL GROWTH OF EUTECTIC Al-Li COMPOSITE MATERIALS[J]. 金属学报, 1996, 32(9): 993-997.
[14] HAO Chuanyong; YU Erjing; YING Huiyun; SHI Chenggen (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). NUCLEATION MECHANISM OF 8090 Al-Li ALLOY WELD METAL[J]. 金属学报, 1996, 32(6): 647-652.
[15] ZHANG Wanming; ZHANG Yun; HU Zhuangqi; LIU Yulin; ZHAO Hong'en;(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-09-15). EFFECTS OF EQUILIBRIUM PHASES ON MECHANICAL PROPERTIES OF 8090 Al-Li ALLOY[J]. 金属学报, 1996, 32(5): 484-488.
No Suggested Reading articles found!