| STRUCTURE AND GLASS FORMING ABILITY (GFA) OF AMORPHOUS ALLOYS |
| LU Ke Institute of Metal Research; Academia Sinica; Shenyang 110015 |
|
Cite this article:
LU Ke Institute of Metal Research; Academia Sinica; Shenyang 110015. STRUCTURE AND GLASS FORMING ABILITY (GFA) OF AMORPHOUS ALLOYS. Acta Metall Sin, 1992, 28(1): 67-76.
|
|
|
Abstract A new microstructure model is developed for amorphous alloys, so called Clus-ter model, in which the amorphous phase is thought of composing of randomly distributed or-dered clusters of different sizes. Thermodynamic calculation on this model deduces a parameter describing the glass forming ability of metallic alloys: a_c=(1-2.08/φm)T_g/ T_m, where T_g is glass transition temperature, T_m is the melting temperature, and φm is entralpy change of melt-ing. It is believed that easy glass forming alloy systems have larger values of a_c This new criter-ion of GFA not only provides the theoretical background for several GFA criteria in the litera-ture cited, but also can predict the GFA of many alloy systems more reasonably and accurately.
|
|
Received: 18 January 1992
|
1 Duwez P, Willens R H, Klement W Jr. J Appl Phys, 1960; 31: 1136 2 Marcus M, Turnbull D. Mater Sci Eng, 1976; 23: 211 3 Donald I W, Davies H A. J Non-Cryst Solids, 1978; 30: 77. 4 Guntherodt H J, Oelhafen P, Lapka R, Kunzi H U, Indlekofer G, Krieg J et al. J Phys (Paris) Colloque, 1980; 41(C8) : 381 5 Sprusil B, Bergmann H W. In: Steeb S, Warlimont H eds., Rapidly Quenched Metals, Amsterdam: North-Holland, 1985: 255 6 Davies H A. In: Cantor B ed., Rapidly Quenched Metals Ⅲ, Vol. Ⅰ, Proc 3rd Int Conf on Rapidly Quenched Metals, London: The Metals Society, 1978: 1 7 Davies H A. In: Luborsky F E ed., Amorphous Metallic Alloys, London: Butterworths, 1983: 8 8 Sommer F, Duddek G, Predel B. Z Metallk, 1978; 69: 587 9 Egami T. In: Luborsky F E ed., Amorphous Metallic Alloys, London: Butterworths, 1983: 100 10 卢柯,王景唐.金属学报,1990;26:B316 11 Fujita F E. In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals 4. Proc 4th Int Conf on Rapidly Quenched Metals, Sendai, August 24--28, 1981, The Japan Institute of Metals, 1982: 301 12 Hamada t, Fujita F E. In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals 4, Proc 4th Int Conf on Rapidly Quenched Metals, Sendai, August 24--28, 1981, The Japan Institute of Metals, 1982: 319 13 Bernal J D. Nature, 1960; 185: 68 Bernal J D. Proc R Soc London, Ser. A, 1964; A280: 299 14 Nishi Y, Suzuki K, Masumoto T. In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals 4, Proc 4th Int Conf on Rapidly Quenched Metals, Sendai, August 24--28, 1981, The Japan Institute of Metals, 1982: 217 15 Nishi Y, Morohoshi T, Kawakami M, Suzuki K, Masumoto T. In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals 4, Proc 4th Int Conf on Rapidly Quenched Metals, Sendai, August 24--28, 1981, The Japan Institute of Metals, 1982: 1113 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|