PREDICTION ABOUT THERMODYNAMIC PROPERTIES OF TERNARY LIQUID ALLOYS FROM WILSON EQUATION |
TAO Dongping Kunming Institute of Technology |
|
Cite this article:
TAO Dongping Kunming Institute of Technology. PREDICTION ABOUT THERMODYNAMIC PROPERTIES OF TERNARY LIQUID ALLOYS FROM WILSON EQUATION. Acta Metall Sin, 1991, 27(6): 92-98.
|
Abstract An attempt was made on applying the Wilson equation to predict the thermodynamic properties of ternary liquid alloys. The activity of each component in ternary liquid alloys was found to be conveniently calculated from the equation with the related binary bimolecular interaction parameters. The calculated values are in fair agreement with experimental data, and are verified to be reliable by the criterion of classical thermodynamics.
|
Received: 18 June 1991
|
1 Prausnitz J M, Lichtenthaler R N, De Azevedo E G. Molecular Thermodynamics of Fluid-Phase Equilibria. 2nd ed., Englewook Cliffis N J: Prentice-Hall Inc., 1986 2 Kellogg H H, Kim Y H, Stapurewicz T. In: Kudryk V, Rao Y K eds., Physical Chemistry of Extractive Metallurgy. New York: AIME, 1985: 3 3 Wilson G M. J Am Chem Soc, 1964; 86: 127 4 Flory P J. J Chem Phys, 1941; 9: 660 5 Huggins M L. J Chem Phys, 1941; 9: 440 6 Elliott J F, Chipman J. J Am Chem Soc, 1951; 73: 2682 7 Mellgren S. J Am Chem Soc, 1952; 74: 5037 8 魏寿昆.活度在冶金物理化学中的应用,北京:中国工业出版社,1964 9 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K. Selected Values of the Thermo dynamic Properties of Binary Alloys, Metals Park, Ohio: ASM, 1973 10 谢冬生.北京钢铁学院学报,1988;10:226 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|