PHASE DIAGRAMS OF BINARY SYSTEMS SmCl_3-Cal_2 and SmCl_3-LiCl |
ZHANG Yifeng;MENG Bo;GU Yunyan Northeast University of Technology; Shenyang |
|
Cite this article:
ZHANG Yifeng;MENG Bo;GU Yunyan Northeast University of Technology; Shenyang. PHASE DIAGRAMS OF BINARY SYSTEMS SmCl_3-Cal_2 and SmCl_3-LiCl. Acta Metall Sin, 1991, 27(6): 150-151.
|
Abstract The phase diagrams of binary systems SmCl_3-CaCl_2 and SmCl_3-LiCl was determined by DTA and X-ray diffraction analysis. The system SmCl_3-CaCl_2 is of a simple eutectic type with eutectic point of 55.8 mol-% SmCl_3 at 545℃. The system SmCl_3-LiCl is of the type with incongruent melting phase 2SmCl_3·LiCl at peritectic point 434℃ and with eutectic point of 31.5 mol-% SmCl_3 at 395℃.
|