EFFECT OF RARE EARTH ON MIDDLE-TEMPERATURE INTERNAL FRICTION OF COMMERCIALLY PURE IRON
JI Jingwen;LAI Zuhan;WU Yuqin;ZHANG Guofu Northeast University of Technology; Shenyang; LI Guangyi Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

JI Jingwen;LAI Zuhan;WU Yuqin;ZHANG Guofu Northeast University of Technology; Shenyang; LI Guangyi Institute of Metal Research; Academia Sinica; Shenyang. EFFECT OF RARE EARTH ON MIDDLE-TEMPERATURE INTERNAL FRICTION OF COMMERCIALLY PURE IRON. Acta Metall Sin, 1991, 27(6): 14-20.

Download:  PDF(679KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of rare earth on the middle-temperature internal friction of commercially pure iron is closely related to heat treatment. The rare earth additive was resulted for acting on alloying. The Snoek-Ke-Koster (briefly called SKK) peak is found to remain still even if the deformed iron after furnace cooling has undergone to age at 600℃ for 1h. The SKK peak temperature does not simply fall as the ascending of aging temperature, but raise up again at 600℃ aging.
Key words:  JI Jingwen      associate professor      Department of Physics      Northeast University of Technology      Shenyang 110006     
Received:  18 June 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I6/14

1 戢景文,魏全金,耿殿奇,吴玉琴.金属学报,1990;26:A14
2 戢景文,赵增祺,贺礼端,耿殿奇.物理学报,1985;34:1620
3 余家森,褚幼义,贺信莱,杜国雄,高佩钰,朱逢吾.钢中稀土.北京:冶金工业出版社,1982:66-71
4 魏全金,戢景文,张国福,赖祖涵.中国稀土学报,待发表
5 吴玉琴,戢景文,赖祖涵.东北工学院学报,1991待发表
6 由淼,杨继先,陈德源.物理学报,1974;23:292
7 葛庭燧,容保粹,王业宁.物理学报,1955;11:91
8 Mura T. In: Ashby M F, Bulough R, Hartley C S, Hirth J P eds., Dislocation Modelling of Physical Systems, Proc Int Conf, Gainesville, Florida, USA, 22--27 June, 1980, Oxford: Pergamon, 1981: 357--367
9 Ino H, Sugeno T. Acta Metall. 1967; 15: 1197
10 包头冶金研究所.稀土应用论文汇编,基础研究部分,冶金工业部钢铁司,1965:40
11 Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids, New York: Academic, 1972X
[1] LIU Junmin; ZHANG Jinxiu (Zhongshan University; Guangzhou 510275)(Manuscript received 1995-08-09; in revised form 1996-04-11). BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION[J]. 金属学报, 1996, 32(8): 785-790.
[2] Acta Metallurgica Sinica<1985.01>. [J]. 金属学报, 1985, 21(1): 9-24.
No Suggested Reading articles found!