DETERMINATION OF DIFFUSION COEFFICIENT OF CuCl_2 IN AQUEOUS SOLUTIONS
WU Zhichun Institute of Chemical Metallurgy; Academia Sinica; Beijing
Cite this article: 

WU Zhichun Institute of Chemical Metallurgy; Academia Sinica; Beijing. DETERMINATION OF DIFFUSION COEFFICIENT OF CuCl_2 IN AQUEOUS SOLUTIONS. Acta Metall Sin, 1991, 27(4): 93-99.

Download:  PDF(556KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The diffusion coefficients of CuCl_2 in aqueous solutions of CuCl_2 andCuCl_2-HCl were measured respectively at 298 K with diaphram cell method. Theconcentration dependency of CuCl_2 diffusion coefficient in single CuCl_2 solution andin mixed CuCl-2-HCl solutions was discussed on the changes in chemical potential aswell as in viscosity.
Key words:  CuCl_2      diffusion coefficient      diaphram cell     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/93

1 Robinson R A, Stokes R H. Electrolyte Solutions, 2nd ed, London: Butterworth's Scientific Publications, 1959
2 Awakuta Y, Ebata A, Morita M, Kondo Y. Denki Kagaku, 1975; 43: 569
3 Filinovsky V Y, Pleskov Y V. In: Yeager E, Bockris J O'M, Couway B E, Sarangapani S eds., Comprehensive Treatise of Electrochemistry, Vol.9, New York: Plenum Press, 1984: 311
4 Johnson S K, Pytkowicz R M. In: Pytkowicz R M ed., Activity Coefficients in Electrolyte Solutions, Vol.2, Boca Raton, FL: CRC Press, 1979: 1--62
5 李皓月,郑蒂基,傅崇说.中南矿冶学院学报,1982;(3) :39
6 Kawasaki U. Master of Engineering Thesis, Kyoto University, Kyoto, Japan. 1987.
[1] Yuanrong LIU,Weimin CHEN,Ying TANG,Yong DU,Lijun ZHANG. APPLICATION OF PRAGMATIC NUMERICAL INVERSE METHOD IN COMPUTATION OF INTERDIFFUSION COEFFICIENTS IN Al TERNARY ALLOYS[J]. 金属学报, 2016, 52(8): 1009-1016.
[2] Zujiang HUANG, Min ZHOU, Yang YANG, Quanzhi CHEN, Shiguang TANG, Weizhou LI. STUDY OF ANODIC ALUMINUM OXIDE FILM AS AN INTERLAYER TO SUPPRESS ELEMENT DIFFUSION[J]. 金属学报, 2016, 52(3): 341-348.
[3] ZHANG Jinling1,2,3, FENG Zhiyong1, HU Lanqing1,2,3,WANG Shebin1,2,3, XU Bingshe1,2,3. PRECIPITATION BEHAVIOR OF AZ91 MAGNESIUM ALLOYS WITH DIFFERENT La CONTENTS[J]. 金属学报, 2012, 48(5): 607-614.
[4] . PHASE FIELD SIMULATION OF SINTERING PROCESS IN BIPHASIC POROUS MATERIAL[J]. 金属学报, 2012, 48(10): 1207-1214.
[5] CHEN Yexin CHANG Qinggang. EFFECT OF TRAPS ON DIFFUSIVITY OF HYDROGEN IN 20g CLEAN STEEL[J]. 金属学报, 2011, 47(5): 548-552.
[6] . The distribution and diffusion of carbon atoms during deformation of undercooled austenite in medium carbon steel[J]. 金属学报, 2007, 43(8): 785-790 .
[7] LIU Shi; ZHENG Hua; GUI Quanhong; MA Aihua; YU Hongbo; WANG Longbao. MEASUREMENTS OF HYDROGEN DIFFUSION COEFFICIENT FOR TUBE SAMPLES AT MEDIUM AND HIGH TEMPERATURES[J]. 金属学报, 2004, 40(4): 393-398 .
[8] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[9] YANG Qiqin; (Department of Chemistry; Zhongshan University; Guangzhou 510275) QIU Kairong; LIU Guankun; GUAN Tong(Zhongshan University;Guangzhou 510275). ELECTROCHEMICAL BEHAVIOUR FOR REDUCTION OF Tm~(3+) IN MOLTEN CHLORIDES[J]. 金属学报, 1995, 31(22): 445-450.
[10] WANG Wendong; ZHANG Sanhong; HE Xinlai(University of Science and Technology Beijing; 100083)(Manuscript received 93-09-21. in revised form 94-01-26). DIFFUSION OF BORON IN Fe-BASE AND Ni-BASE ALLOYS[J]. 金属学报, 1995, 31(2): 56-63.
[11] ZHU Xiaohe;YU Yongning University of Science and Technology Beijing. DIFFUSION COEFFICIENTS IN α(δ)-PHASE OF Fe-Mn-Si TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1991, 27(3): 106-110.
[12] YANG Zhen'guo;DU Weixi;DU Senlin;LIU Sulan Jilin University of Technology; Changchun Changchun Institute of Applied Chemistry; Academia Sinica. DIFFUSION OF La IN LIQUID Al-Si ALLOY[J]. 金属学报, 1989, 25(2): 104-108.
No Suggested Reading articles found!