Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (3): 33-40    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF SELF-ACCOMMODATION FOR TWINNED MARTENSITE AND INVARIANT HABIT PLANE
GU Nanju;WANG Ruixiang;YIN Fuxing Hebei Institute of Technology; Tianjin
Cite this article: 

GU Nanju;WANG Ruixiang;YIN Fuxing Hebei Institute of Technology; Tianjin. EFFECT OF SELF-ACCOMMODATION FOR TWINNED MARTENSITE AND INVARIANT HABIT PLANE. Acta Metall Sin, 1991, 27(3): 33-40.

Download:  PDF(602KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The shear components of strain tensors for matrix and twin crystal oftwinned martensite were opposite roughly after calculation, and the strain energywould be reduced. The growth of martensitic plates along the normal direction ofthe twin plane may depend upon the effect of self-accommodation between the ma-trix and twin crystals. Based upon the analysis on the displacement vectors of thenormals for different habit planes, the {10,3,15}_f plane could make up the macro-scopic invariant habit planes; but the (575)_f, (252)_f, (111)_f planes are difficult tobecome the invariant planes.
Key words:  self-accommodation      invariant habit plane      displacement vector     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/33

1 Wayman C M. Introduction to the Crystallography of Martensitic Transformations. New York: The Macmillan Company, 1964
2 Otsuka K. Proc Int Conf on Martensitic Transformations, Nara, Japan, 1986: 35--42
3 Kajiwara S. Trans Jpn Inst Met, 1976: 17: 435
4 李永森.金属学报,1986;22:B212,B221
5 蒋正行.金属科学与工艺.1984;3(3) :36
6 Gu Nanju. Proc Int Conf on Martensitic Transformations, Nara. Japan, 1986: 325--330
7 李春志.物理学报,1979;28(3) :314
8 Zhang Xiumu, Gautier E. Acta Metall, 1989; 37: 491
9 Schroeder T A, Wayman C M. Acta Metall, 1977; 25: 1375
10 Saburi T, Wayman C M. Acta Metall, 1980; 28: 15--32m
[1] MAN Jiao ZHANG Jihua RONG Yonghua. THREE-DIMENSIONAL PHASE FIELD STUDY ON STRAIN SELF-ACCOMMODATION IN MARTENSTIC TRANSFORMATION[J]. 金属学报, 2010, 46(7): 775-780.
No Suggested Reading articles found!