| HYDROGEN TRAPPING EFFECT OF SUBSTITUTIONAL ALLOYING ELEMENTS IN α-Fe |
| QIAN Lihe;CAO Mingzhou;WAN Xiaojing Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
QIAN Lihe;CAO Mingzhou;WAN Xiaojing Institute of Metal Research; Academia Sinica; Shenyang. HYDROGEN TRAPPING EFFECT OF SUBSTITUTIONAL ALLOYING ELEMENTS IN α-Fe. Acta Metall Sin, 1991, 27(1): 27-31.
|
|
|
Abstract The effect of Cr, Mn, Co, Ni, Si or Mo on the diffusivity of hydro-gen in α-Fe has been studied near room temperature by means of sensitive electro-chemical method. With the of increases concentration of alloying elements, the hydro-gen diffusivity in binary Fe alloys decreases and the activation energy increases. Onthe basis of Oriani's approach, the trapping parameters of the alloying elements inthe Fe alloys are calculated and the trap binding energy between the above elementsand hydrogen are obtained. The increasing sequence of trap binding energy is asfollows: Si, Co, Ni, Mn, Cr, Mo. Finally, the nature of the trap binding energy isanalyzed according to both the interaction between lattice strain field induced byalloying elements and hydrogen elasticity as well as the interaction between alloy-ing elements and hydrogen electricity.
|
|
Received: 18 January 1991
|
1 Darken L S, Smith R P. Cortosion, 1949; 5: 1 2 Oriani R A. Acta Metall, 1970; 18: 147 3 Pressouyre G M, Bernstein I M. Metall Trans, 1987; 9A: 1571 4 Devanathan M A V, Stachurski Z. Proc R Soc, 1962; A270: 90 5 刁元东,中国科学院金属研究所硕士学位论文,1988 6 Kim K T, Park J K, Lee J Y, Hwang S H. J Mater Sci, 1981; 16: 2590 7 Shirley A I, Hall C K. Ser Metall, 1983; 17: 1003 8 Pressouyre G M. Metall Trans, 1979; 10A: 1571 9 杨柯,中国科学院金属研究所博士学位论文,1989 10 Sigworth G K. Elliott J F. Met Sci, 1974; 8: 298 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|