Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (6): 94-99    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF POTENTIAL ON INTERACTION BETWEEN STRESS CORROSION CRACKING AND CORROSION FATIGUE OF AUSTENITIC STAINLESS STEEL IN BOILING 42% MgCl_2 SOLUTION
FENG Tao;CHEN Liangshi;KE Wei Corrosion Science Laboratory; Academia Sinica; Shenyang
Cite this article: 

FENG Tao;CHEN Liangshi;KE Wei Corrosion Science Laboratory; Academia Sinica; Shenyang. EFFECT OF POTENTIAL ON INTERACTION BETWEEN STRESS CORROSION CRACKING AND CORROSION FATIGUE OF AUSTENITIC STAINLESS STEEL IN BOILING 42% MgCl_2 SOLUTION. Acta Metall Sin, 1990, 26(6): 94-99.

Download:  PDF(1429KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The environment-sensitive fracture behaviour of 0Cr18Ni9Ti austeniticstainless steel in boiling 42% MgCl_2 under the specific load of low frequency andhigh mean stress was investigated from the relations and differences on crack gro-wth rates and fractographys between stress corrosion fatigue and stress corrosioncracking. The interaction between stress corrosi on cracking and corrosion fatiguewas also studied from fracture characteristics, with emphasison the effect of appliedpotential on the interaction.
Key words:  environment-sensitive fracture      stress corrosion cracking      corrosion fatigue      stress corrosion fatigue     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/94

1 Eremias B, Maricev V A. Werks Korros, 1979; 30: 551
2 Staehle R W. In: Miller K J, Smith R F eds., Mechanical Behaviour of Materials, Vol. 1, Proc the 3rd Int Conf, held in Cambridge, England, 20--24 August 1978, Oxford: Pergamon, 1979: 93
3 Gattgher J P, Wei R P. Proc the Int Conf on Corrosion Fatigue: Chemistry, Mechanics and Microstructure, 14--18 June, 1971, Sponsored by National Assn. of Corrosion Engineers, etc. Houston, NACE, 1972: 409
4 Wei R P. In: Gu Haicheng, He Jiawen eds., Proc of an Int Syposium on Microstructure and Mechanical Behaviour of Materials, held in Xi'an. China, 21--24 October, 1985: 507B
[1] MA Zhimin, DENG Yunlai, LIU Jia, LIU Shengdan, LIU Honglei. Effect of Quenching Rate on Stress Corrosion Cracking Susceptibility of 7136 Aluminum Alloy[J]. 金属学报, 2022, 58(9): 1118-1128.
[2] TAN Jibo, WANG Xiang, WU Xinqiang, HAN En-Hou. Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water[J]. 金属学报, 2021, 57(3): 309-316.
[3] Hongchi MA, Cuiwei DU, Zhiyong LIU, Yong LI, Xiaogang LI. Comparative Study of Stress Corrosion Cracking Behaviors of Typical Microstructures of Weld Heat-Affected Zones of E690 High-Strength Low-Alloy Steel in SO2-Containing Marine Environment[J]. 金属学报, 2019, 55(4): 469-479.
[4] Ping DENG,Chen SUN,Qunjia PENG,En-Hou HAN,Wei KE,Zhijie JIAO. Study on Irradiation Assisted Stress Corrosion Cracking of Nuclear Grade 304 Stainless Steel[J]. 金属学报, 2019, 55(3): 349-361.
[5] Jun YU, Deping ZHANG, Ruosheng PAN, Zehua DONG. Electrochemical Noise of Stress Corrosion Cracking of P110 Tubing Steel in Sulphur-Containing Downhole Annular Fluid[J]. 金属学报, 2018, 54(10): 1399-1407.
[6] Hongzhong YUAN,Zhiyong LIU,Xiaogang LI,Cuiwei DU. Influence of Applied Potential on the Stress Corrosion Behavior of X90 Pipeline Steel and Its Weld Joint in Simulated Solution of Near Neutral Soil Environment[J]. 金属学报, 2017, 53(7): 797-807.
[7] Hongliang MING,Zhiming ZHANG,Jianqiu WANG,En-Hou HAN,Mingxing SU. Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW[J]. 金属学报, 2017, 53(1): 57-69.
[8] Maocheng YAN,Shuang YANG,Jin XU,Cheng SUN,Tangqing WU,Changkun YU,Wei KE. STRESS CORROSION CRACKING OF X80 PIPELINE STEEL AT COATING DEFECT IN ACIDIC SOIL[J]. 金属学报, 2016, 52(9): 1133-1141.
[9] Zhiyong LIU,Zongshu LI,Xiaolin ZHAN,Wenzhu HUANGFU,Cuiwei DU,Xiaogang LI. GROWTH BEHAVIOR AND MECHANISM OF STRESS CORROSION CRACKS OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION[J]. 金属学报, 2016, 52(8): 965-972.
[10] Zilong ZHANG, Shuang XIA, Wei CAO, Hui LI, Bangxin ZHOU, Qin BAI. EFFECTS OF GRAIN BOUNDARY CHARACTER ON INTERGRANULAR STRESS CORROSION CRACKING INITIATION IN 316 STAINLESS STEEL[J]. 金属学报, 2016, 52(3): 313-319.
[11] Hongchi MA, Cuiwei DU, Zhiyong LIU, Wenkui HAO, Xiaogang LI, Chao LIU. STRESS CORROSION BEHAVIORS OF E690 HIGH-STRENGTH STEEL IN SO2-POLLUTED MARINE ATMOSPHERE[J]. 金属学报, 2016, 52(3): 331-340.
[12] Ju KANG,Jichao LI,Zhicao FENG,Guisheng ZOU,Guoqing WANG,Aiping WU. INVESTIGATION ON MECHANICAL AND STRESS CORROSION CRACKING PROPERTIES OF WEAKNESS ZONE IN FRICTION STIR WELDED 2219-T8 Al ALLOY[J]. 金属学报, 2016, 52(1): 60-70.
[13] Yueling GUO, En-Hou HAN, Jianqiu WANG. EFFECTS OF FORGING AND HEAT TREATMENTS ON STRESS CORROSION BEHAVIOR OF 316LN STAINLESS STEEL IN HIGH TEMPERATURE CAUSTIC SOLUTION[J]. 金属学报, 2015, 51(6): 659-667.
[14] WU Xinqiang, TAN Jibo, XU Song, HAN En-Hou, KE Wei. CORROSION FATIGUE MECHANISM OF NUCLEAR-GRADE LOW ALLOY STEEL IN HIGH TEMPERATURE PRESSURIZED WATER AND ITS ENVIRONMENTAL FATIGUE DESIGN MODEL[J]. 金属学报, 2015, 51(3): 298-306.
[15] YAN Maocheng, WANG Jianqiu, HAN En-hou, SUN Cheng, KE Wei. CHARACTERISTICS AND EVOLUTION OF THIN LAYER ELECTROLYTE ON PIPELINE STEEL UNDER CATHODIC PROTECTION SHIELDING DISBONDED COATING[J]. 金属学报, 2014, 50(9): 1137-1145.
No Suggested Reading articles found!