FACTORS AFFECTING SILICA CONTENT OF ALUMINIUM HYDROXIDE PRODUCT IN CARBONIZATION PROCESS
LIU Miaoxiu;CHENG Zhaonian;CHEN Nianyi;KE Jiajun Shanghai Institute of Metallurgy; Academia Sinica Institute of Chemical Metallurgy; Academia Sinica; Beijing
Cite this article: 

LIU Miaoxiu;CHENG Zhaonian;CHEN Nianyi;KE Jiajun Shanghai Institute of Metallurgy; Academia Sinica Institute of Chemical Metallurgy; Academia Sinica; Beijing. FACTORS AFFECTING SILICA CONTENT OF ALUMINIUM HYDROXIDE PRODUCT IN CARBONIZATION PROCESS. Acta Metall Sin, 1990, 26(5): 156-159.

Download:  PDF(323KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The regularity of carbonization process for alumina production has been summa-rized by the pattern recognition and regression. A mathematical model has been proposed todescEribe the factors affecting the silica content of aluminium hydroxide product. The high con-ecranttion of aluminate ion in solution will prodoce aluminuium hydroxide with low content ofSiO_2 under the condition of Al_2O_3/SiO_2 ratio kept unchanged. This was confirmed by the auth-ors′certain scale experiments.KEY
Key words:  carbonization      silica content      alumina production      pattern recognition     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/156

1 Chen Nianyi. Anal Chim Acta, 1988; 210: 175
2 陈念贻.计算化学及其应用,上海科技出版社,1987
3 程兆年,汤峰潮,罗学才,张未名,陈念贻.化工学报 待发表
4 程兆年,汤峰潮,陈念贻.计算机与应用化学,1989;6:7
5 张未名,陈念贻,李再琮,李建平,茅仁杰.自动化学报,1989;15:1
6 Geladi P. Kowalski B R. Anal Chim Acta, 1986; 185: 1
7 Wold S. Pattern Recognition, 1976; 8:127
8 Sammon J W. IEEE Trans Comput, 1970; C--19: 826
9 Guth J L, Caullet P, Jacques P, Wey R. Bull Soc Chim Fr, 1980; (3--4) : Ⅰ--122
10 柳妙修,周佩芳,陈念贻,柯家骏.金属学报 待发
[1] WEI Jie, WEI Yinghua, LI Jing, ZHAO Hongtao, LV Chenxi, DONG Junhua, KE Wei, HE Xiaoyan. Corrosion Behavior of Damaged Epoxy Coated Steel Bars Under the Coupling Effect of Chloride Ion and Carbonization[J]. 金属学报, 2020, 56(6): 885-897.
[2] ZHANG Peng ZHANG Fucheng WANG Tiansheng. PREPARATION AND MICROSTRUCTURE OF HARD BAINITE IN SURFACE LAYER OF CARBURIZED 20CrMnMoAl STEEL[J]. 金属学报, 2011, 47(8): 1038-1045.
[3] WANG Lei ZHANG Sixun DONG Junhua KE Wei LIU Chunming . SURFACE CRAZING OF Mn–Cu WEATHERING STEEL[J]. 金属学报, 2010, 46(6): 723-728.
[4] WU Xiaojun CHENG Wen QIAO Shengru ZOU Wu ZHANG Peng ZHANG Xiaohu. EVOLUTION OF PORES IN C/C COMPOSITE DURING RESIN IMPREGNATION-CARBONIZATION[J]. 金属学报, 2009, 45(11): 1402-1408.
[5] WANG Zhi; BI Shiwen; YANG Yihong. Effects of Additives on Particle Size and Strength of Carbonization Product in Sodium Aluminate Liquors[J]. 金属学报, 2004, 40(9): 1005-1008 .
[6] ZHANG Xiaoqing; SUN Yongqing; ZHANG Zheng. Recognition of Metal Fracture Surface Morphologies Based on the Fuzzy Texture Spectrum[J]. 金属学报, 2004, 40(10): 1018-1022 .
[7] ZHANG Zhaochun; WU Zhu; LI Chonghe; QIN Pei; CHEN Nianyi(Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050)Correspondent: WU Zhu; Tel: (021)62511070-8932; Fax: (021)62513510. APPLICATION OF PATTERN RECOGNITION AND ARTIFICIAL NEURAL NETWORK TO IMPROVE THE MECHANICAL PROPERTIES OF CYLINDER BLOCK CAST OF AUTOMOBILE ENGINE[J]. 金属学报, 1998, 34(10): 1068-1072.
[8] CONG Peisheng; LI Tonghua (Tongji University; Shanghai) CHEN Yu; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Sinica; Shanghai). NEURON ADAPTIVE ALGORITHM APPLIED TO EXPERIMENTAL DESIGN IN STEEL PRODUCTION[J]. 金属学报, 1992, 28(11): 59-61.
[9] ZHOU Diangen; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Sinica; Shanghai). PATTERN RECOGNITION APLLIED TO STABILITY OF FILLED Ti_2Ni PHASES[J]. 金属学报, 1992, 28(11): 20-22.
[10] CHEN Yu; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Sinica)PENG Ping; KONG Bingyu (Iron and Steel Research Institute; Shanghai Baoshan Iron and Steel Complex). ASPRES—AN EXPERT SYSTEM FOR ALLOY STEEL DEVELOPMENT[J]. 金属学报, 1992, 28(10): 91-94.
No Suggested Reading articles found!