Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (3): 55-60    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF GRAIN BOUNDARY ON FATIGUE BEHAVIOUR OF Al BICRYSTALS
LI Qingsheng (Chingshen Li);T. BRETHEAU Taiyuan University of Technology University Paris Nord Department of Mathematics and Mechanics;Taiyuan University of Technology; Taiyuan 030024
Cite this article: 

LI Qingsheng (Chingshen Li);T. BRETHEAU Taiyuan University of Technology University Paris Nord Department of Mathematics and Mechanics;Taiyuan University of Technology; Taiyuan 030024. EFFECT OF GRAIN BOUNDARY ON FATIGUE BEHAVIOUR OF Al BICRYSTALS. Acta Metall Sin, 1990, 26(3): 55-60.

Download:  PDF(1293KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of grain boundaries on cyclic deformation and fatiguecrack growth in Al bicrystals under stress controlling in laboratory atmospherehas been studied. The effect of a grain boundary is found to be restricted in anarrow area, termed as grain boundary affecting zone (GBAZ), where the incom-patible plastic strain by the two sides of the interface under cyclic loads creats in-ternal stress which conversely promotes inhomogeneous slip in the area and grainboundary cracking. As an extended stage I crack initiated from a notch approachesthe grain boundary under a constant cyclic load, the crack branches, the crackfront splits into several pieces, meanwhile, the growth rate reduces to a minimumvalue at the centre of GBAZ. Such microstructure-sensitive growth of extendedstage I cracks is mainly attributed to the grain boundary-induced crack tip shielding.
Key words:  compatibity      growth stage I      crack tip shielding      crack tip displacement     
Received:  18 March 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I3/55

1 Clark R, Chalmers B. Acta Metall, 1954; 2: 80
2 Miller K J. Fatigue Fract Eng Mater Struct, 1987; 10: 75
3 Chuang Y D, Margolin H. Metall Trans, 1973; 4A: 1905
4 Jayaram V. Acta Metall, 1982; 33: 1307
S Rey C, Zaoui A. Acta Metall, 1980; 28: 687
6 Nageswarao M, Gerold V. Metall Trans, 1976; 7A: 1847
7 Li C, Bretheau T. Proc 7th Int Conf on Fracture. Huston, 1989
8 Chan K S. Acta Metall, 1987; 35: 981
9 Suresh S, Ritchie R O. Metall Trans, 1982; 13A: 1627
10 Pande C S, Masumura R A, Chou Y T. Acta Metall, 1988; 36: 49
11 Weertman J, Hack J E. Int J Fract, 1988; 34: 27
12 Li C. Fatigue Fract Eng Mater Struct, 1989; 12: 59
[1] CHEN Zheng Northwestern Polytechnical University; Xi'an. THRESHOLD OF SHORT FATIGUE CRACK FOR 8090 Al-Li ALLOY[J]. 金属学报, 1990, 26(5): 62-65.
No Suggested Reading articles found!