| PREPARATION OF ULTRAFINE PARTICLES OF Fe AND ZrO_2 WITH METASTABLE PHASES BY HIGH POWER LASER BEAMS |
| XU Huibin;TAN Shusong Technische Universitat Berlin. FRG Department of Materials;Central South University of Technology; Changsha 410083 |
|
Cite this article:
XU Huibin;TAN Shusong Technische Universitat Berlin. FRG Department of Materials;Central South University of Technology; Changsha 410083. PREPARATION OF ULTRAFINE PARTICLES OF Fe AND ZrO_2 WITH METASTABLE PHASES BY HIGH POWER LASER BEAMS. Acta Metall Sin, 1990, 26(2): 152-155.
|
|
|
Abstract The radiation of material surface by high intensity laser beams is used to producethe ultrafine powder of pure Fe and ZrO_2. The morphology, the size and the phases of the pow-der were examined by X-ray diffractometer, scanning electron microscopy as well as transmis-sion electron microscopy. In the pure Fe a considerable quantity of γ-phase was found in thepowder. In ZrO_2 powder, instead of stable phase, two metastable phases appeared.
|
|
Received: 18 February 1990
|
1 Van Stone R H, Rizzo F J, Raisch J F. In: Mehrabian R, Kear B H, Cohen M eds., Rapid Solidification Processing: Priciples and Technologies II, Baton Rouge: Claitor's Publishing Division, 1980: 260 2 Gleiter H, Marquardt P. Z Metallk, 1984; 75: 263 3 Fukano Y. Jpn J Appl Phys, 1974; 13: 1001 4 Kato M, Mori T. Acta Metall, 1977; 25: 951 5 Teufer G. Acta Crystallogr, 1962; 15: 118 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|